Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group ORGASOL® 2002 ES 6 Nat 3 Polyamide 12

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer Arkema
Trade Name ORGASOL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group ORGASOL® 2002 ES 6 Nat 3 Polyamide 12.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Arkema Group
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ISO 1183
Apparent Bulk Density 0.425 g/cc
0.0154 lb/in³
ISO 1068
Particle Size 57 - 63 µm
57 - 63 µm
Average; ATO 40-41-0 (Coulter Counter)
pH >= 4.0
>= 4.0
ATO 40-40-0 (pH meter)
Specific Surface Area 1.0 m²/g
1.0 m²/g
ATO 40-45-0 (BET)
Thermal Properties Metric English Comments
Melting Point 177 °C
351 °F
ISO 3146
Processing Properties Metric English Comments
Moisture Content 1.0 %
1.0 %
ISO 1625