Arkema Group OREVAC® 18334 Grafted Maleic Anhydride Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , Anhydride-Modified Polyethylene
Manufacturer Arkema
Trade Name OREVAC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group OREVAC® 18334 Grafted Maleic Anhydride Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
OREVAC 18334 is a grafted maleic anhydride polyethylene used in the manufacturing of multilayer oxygen barrier bottle. OREVAC 18334 is mainly used in multi-layer bottle and tank to have good adhesion between PEHD, PA and EVOH. OREVAC 18334 combined with SOARNOL® from NIPPON GOSHEI provides very good oxygen barrier. These structures are used in milky products conditionings, fuel tanks and also industrial applications.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.920 g/cc

@Temperature 23.0 °C
0.0332 lb/in³

@Temperature 73.4 °F
ISO 1183
Melt Index of Compound 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 45
45
ISO 868
Tensile Strength at Break 30.0 MPa
4350 psi
ASTM D638
Tensile Strength, Yield 4.50 MPa
653 psi
ASTM D638
Elongation at Break 760 %
760 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 125 °C
257 °F
DSC
Vicat Softening Point 95.0 °C

@Load 0.999 kg
203 °F

@Load 2.20 lb
ISO 306