SABIC Innovative Plastics LNP LUBRICOMP DL001 PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP DL001 PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* LUBRICOMP* DL001 is a compound based on Polycarbonate resin containing PTFE. Added features include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 57.0 MPa
8270 psi
5 mm/min; ISO 527
Elongation at Yield 5.6 %
5.6 %
5 mm/min; ISO 527
Tensile Modulus 2.30 GPa
334 ksi
1 mm/min; ISO 527
Flexural Yield Strength 91.0 MPa
13200 psi
2 mm/min; ISO 178
Flexural Modulus 2.30 GPa
334 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*4; ISO 180/1A
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 74.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
41.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 73.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
40.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
280 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 128 °C
262 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 V-1

@Thickness 3.00 mm
V-1

@Thickness 0.118 in
UL 94