Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 45.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 35.0 - 45.0 MPa
5080 - 6530 psi
ASTM D638-03
Proto3000 Objet Digital Materials™ DM_8425 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide..
Tensile Strength at Break 35.0 - 45.0 MPa
5080 - 6530 psi
ASTM D638-03
Proto3000 Objet Digital Materials™ DM_8505Gray50 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr..
Tensile Strength at Break 40.0 - 45.0 MPa
5800 - 6530 psi
ASTM D683
Loxim 820 01 HB Polypropylene Compound, Flame Retardant
Information provided by Loxim Industries
Tensile Strength at Break 20.0 - 45.0 MPa
2900 - 6530 psi
ASTM D638
Daikin POLYFLON F-104 PTFE Fine Powder
Processing Methods: Paste extrusion, calendering.Applications: Unsintered tape, sealing tape, low specific gravity tape, tape for wrapping flat cables, tubes.Information provided by Daikin Industrie..
Tensile Strength at Break 20.0 - 45.0 MPa
2900 - 6530 psi
ASTM D638
Daikin POLYFLON F-201 PTFE Fine Powder
Processing Methods: Paste extrusion.Applications: Spaghetti tubes, small diameter tubes, fine electric wire smaller than AGW16.Information provided by Daikin Industries.
Tensile Strength at Break 20.0 - 45.0 MPa
2900 - 6530 psi
ASTM D638
Daikin POLYFLON F-205 PTFE Fine Powder
Processing Methods: Paste extrusion.Applications: Spaghetti tubes, small diameter tubes, fine electric wire smaller than AGW16.Information provided by Daikin Industries.
Tensile Strength at Break 20.0 - 45.0 MPa
2900 - 6530 psi
ASTM D638
Daikin POLYFLON F-302 PTFE Fine Powder
Processing Methods: Paste extrusion.Applications: Small to large diameter tubes, flexible hoses, shrinkable tubes, heavy duty electric wires smaller than AGW18, and jackets.Information provided by ..
Tensile Strength at Break 20.0 - 45.0 MPa
2900 - 6530 psi
ASTM D638
Daikin POLYFLON M-111 PTFE Molding Powder, Fine Cut
Fine cut powder.Processing Methods: Compression molding.Features: Produces moldings with extremely smooth and fine surface. Suited to making packing and gaskets since moldings have an especially go..
Tensile Strength at Break 20.0 - 45.0 MPa
2900 - 6530 psi
ASTM D638
Daikin POLYFLON M-112 PTFE Molding Powder, Fine Cut
Fine cut powder.Processing Methods: Compression molding.Features: Produces moldings with especially good elasticity, making it ideal for molding diaphragms and bellows. Offers excellent post-moldin..
Tensile Strength at Break 20.0 - 45.0 MPa
2900 - 6530 psi
ASTM D638
Daikin POLYFLON M-12 PTFE Molding Powder, Fine Cut
Fine cut powder.Processing Methods: Compression molding.Features: Useful in making products requiring fine texture, especially insulation skiving tapes. Also allows uniform mixing of inorganic fill..
Tensile Strength at Break 20.0 - 45.0 MPa
2900 - 6530 psi
ASTM D638
Daikin POLYFLON M-139 PTFE Molding Powder, Free Flow
Free flow powder.Processing Methods: Compression molding and automatic compression molding.Features: Excellent fluidity. Apparent density is large and ideal for automated compression molding proces..
Tensile Strength at Break 20.0 - 45.0 MPa
2900 - 6530 psi
ASTM D638
Daikin POLYFLON M-18 PTFE Molding Powder, Fine Cut
Fine cut powder.Processing Methods: Compression molding.Features: Suited to molding of large billets, has nearly the same molding characteristics of M-12. Also allows uniform mixing of inorganic fi..
Tensile Strength at Break 20.0 - 45.0 MPa
2900 - 6530 psi
ASTM D638
Daikin POLYFLON M-391 PTFE Molding Powder, Free Flow
Free flow powder.Processing Methods: Compression molding and automatic or semi-automatic compression molding.Features: Used if concerned about insufficient molding pressure for flat sheets.Informati..
Tensile Strength at Break 20.0 - 45.0 MPa
2900 - 6530 psi
ASTM D638
Daikin POLYFLON M-392 PTFE Molding Powder, Free Flow
Free flow powder.Processing Methods: Compression molding, automatic or semi-automatic compression molding, isostatic molding, and ram extrusion.Features: Good fill characteristics particularly into ..
Tensile Strength at Break 20.0 - 45.0 MPa
2900 - 6530 psi
ASTM D638
Daikin POLYFLON M-393 PTFE Molding Powder, Free Flow
Free flow powder.Processing Methods: Compression molding, automatic compression molding, and ram extrusion.Features: Maximum emphasis given to ease of handling during molding. Used when molded arti..
Tensile Strength at Break 20.0 - 45.0 MPa
2900 - 6530 psi
ASTM D638
Daikin POLYFLON MG-1030 PTFE 15% Glass Fiber Filled Molding Powder
15% glass fiber filled. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Available in all forms (e.g. bearings, gaskets, valve seats,..
Tensile Strength at Break 20.0 - 45.0 MPa
2900 - 6530 psi
ASTM D638
Daikin POLYFLON MG-1040F PTFE 20% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow
20% glass fiber filled. High apparent density and free-flowing properties. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Availabl..
Tensile Strength at Break 20.0 - 45.0 MPa
2900 - 6530 psi
ASTM D638
Daikin POLYFLON MG-1050F PTFE 25% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow
25% glass fiber filled. High apparent density and free-flowing properties. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Availabl..
Tensile Strength at Break 20.0 - 45.0 MPa
2900 - 6530 psi
ASTM D638
Daikin POLYFLON MG-1241 PTFE 20% Glass Fiber and 5% Graphite Filled Molding Powder
20% glass fiber and 5% graphite filled. High wear resistance, low friction, high creep resistance.Applications: Mechanical and chemical service (e.g. piston rings, bearing pads, and packings)Inform..
Tensile Strength at Break 20.0 - 45.0 MPa
2900 - 6530 psi
ASTM D638
Daikin POLYFLON MG-1241F PTFE 20% Glass Fiber and 5% Graphite Filled Molding Powder, High Apparent Density, Free Flow
20% glass fiber and 5% graphite filled. High apparent density and free-flowing properties. High wear resistance, low friction, high creep resistance.Applications: Mechanical and chemical service (..
Tensile Strength at Break 20.0 - 45.0 MPa
2900 - 6530 psi
ASTM D638
Daikin POLYFLON MG-1431 PTFE 15% Glass Fiber and 5% MoS2 Filled Molding Powder
15% glass fiber and 5% MoS2 filled. High wear resistance, good electrical properties, low friction, high creep resistance.Applications: Mechanical and electrical service (e.g. split-curled bearings..
Tensile Strength at Break 20.0 - 45.0 MPa
2900 - 6530 psi
ASTM D638
Daikin POLYFLON MG-1431F PTFE 20% Glass Fiber and 5% MoS2 Filled Molding Powder, High Apparent Density, Free Flow
15% glass fiber and 5% MoS2 filled. High apparent density and free-flowing properties. High wear resistance, good electrical properties, low friction, high creep resistance.Applications: Mechanica..
Tensile Strength at Break 20.0 - 45.0 MPa
2900 - 6530 psi
ASTM D638
Daikin POLYFLON MG-2030 PTFE 15% Graphite Filled Molding Powder
15% graphite filled. Low friction, excellent chemical resistance, high creep resistance.Applications: Mechanical and chemical service (e.g. bearings, gaskets, packings)Information provided by Daiki..
Tensile Strength at Break 20.0 - 45.0 MPa
2900 - 6530 psi
ASTM D638
Daikin POLYFLON MG-6030 PTFE 15% Carbon Fiber Filled Molding Powder
15% carbon fiber filled. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechanical seals and bearing pads)Information provided by ..
Tensile Strength at Break 20.0 - 45.0 MPa
2900 - 6530 psi
ASTM D638
Daikin POLYFLON MG-6030F PTFE 15% Carbon Fiber Filled Molding Powder, High Apparent Density, Free Flow
15% carbon fiber filled. High apparent density and free-flowing properties. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechan..
Tensile Strength at Break 20.0 - 45.0 MPa
2900 - 6530 psi
ASTM D638
Daikin POLYFLON MG-6050 PTFE 25% Carbon Fiber Filled Molding Powder
25% carbon fiber filled. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechanical seals and bearing pads)Information provided by ..
Tensile Strength at Break 20.0 - 45.0 MPa
2900 - 6530 psi
ASTM D638
Daikin POLYFLON MG-1030F PTFE 15% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow
15% glass fiber filled. High apparent density and free-flowing properties. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Availabl..
Tensile Strength at Break 20.0 - 45.0 MPa
2900 - 6530 psi
ASTM D638
Daikin POLYFLON MG-1050 PTFE 25% Glass Fiber Filled Molding Powder
25% glass fiber filled. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Available in all forms (e.g. bearings, gaskets, valve seats,..
Tensile Strength at Break 30.0 - 45.0 MPa
4350 - 6530 psi
5 mm/min.; IS 867-1963
Amity Thermosets ATE 183 M Phenolic Molding Mica and organic Filler, Compression Molded
Characteristics:Electric low loss Low water absorption Low shrinkage Heat stableGlossy surface finishVery good mouldabilityGood electrical insulationGood chemical resistantColor-blackMedium flowAppl..
Tensile Strength at Break 30.0 - 45.0 MPa
4350 - 6530 psi
5 mm/min.; IS 867-1963
Amity Thermosets ATE 183 Phenolic Molding Mica and organic Filler, Compression Molded
Characteristics:Electric low loss Low water absorption Low shrinkage Heat stableGlossy surface finishVery good mouldabilityGood electrical insulationGood chemical resistantColor-blackMedium flowAppl..