Category | Metal , Electronic/Magnetic Alloy , Nonferrous Metal , Cobalt Alloy |
Manufacturer | Alliance LLC |
Trade Name | |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Alliance S-22A Samarium Cobalt Magnetic Material.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.40 g/cc | 0.303 lb/in³ |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Vickers | 550 | 550 | |
Modulus of Elasticity | 110 GPa | 16000 ksi | |
Flexural Strength | 120 MPa | 17400 psi | |
Compressive Strength | 1000 MPa | 145000 psi |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 7.00 µm/m-°C @Temperature 20.0 °C |
3.89 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
CTE, linear, Transverse to Flow | 13.0 µm/m-°C @Temperature 23.0 °C |
7.22 µin/in-°F @Temperature 73.4 °F |
|
Specific Heat Capacity | 0.370 J/g-°C | 0.0884 BTU/lb-°F | |
Thermal Conductivity | 10.0 W/m-K | 69.4 BTU-in/hr-ft²-°F | |
Maximum Service Temperature, Air | 250 °C | 482 °F |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000500 - 0.0000600 ohm-cm | 0.0000500 - 0.0000600 ohm-cm | |
Magnetic Coercive Force, Hc | 9100 Oe | 9100 Oe | |
16000 Oe | 16000 Oe | Intrinsic | |
Magnetic Remanence, Br | 9500 Gauss | 9500 Gauss | |
Magnetic Maximum Energy Product, BH | 22 MGOe | 22 MGOe | |
Curie Temperature | 750 °C | 1380 °F |
Descriptive Properties | Value | Comments |
---|---|---|
Reversible Temp Coef., Bd | -0.05 %/°C | |
Reversible Temp Coef., Hd | +0.25 %/°C | |
Temperature Coefficient, Br | -0.04 %/°C | (20-100°C) |
Temperature Coefficient, Hci | -0.045 %/°C | (20-100°C) |