Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Albis Plastics Tedur® P 9519 PPS, ~45% Glass Fiber (black only)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler
Manufacturer Albis Plastics
Trade Name Tedur®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Albis Plastics Tedur® P 9519 PPS, ~45% Glass Fiber (black only).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Compounded Regrind and/or Production Scrap, Excellent Cost-Performance Ratio. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Handles, Fixing ElementsProcessing: Injection Molding (Melt Temperature: 610-645°F, Mold Temperature: 285°F)Tedur® is manufactured by Albis Plastics Corporation under license of the registered trademark owner (Bayer.) Data supplied by Albis Plastics Corporation.
Physical Properties Metric English Comments
Density 1.70 g/cc
0.0614 lb/in³
DIN 53 47
Mechanical Properties Metric English Comments
Tensile Strength at Break 165 MPa
23900 psi
DIN 53 455
Elongation at Break 1.6 %
1.6 %
DIN 53 455
Modulus of Elasticity 16.0 GPa
2320 ksi
DIN 53 457
Flexural Yield Strength 240 MPa
34800 psi
DIN 53 452
Flexural Modulus 14.0 GPa
2030 ksi
DIN 53 457
Izod Impact, Notched 2.99 J/cm
5.60 ft-lb/in
Approximation; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ASTM D648
Flammability, UL94 V-0
V-0
Albis North America Internal Test
Processing Properties Metric English Comments
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Mold Temperature 141 °C
286 °F
Users viewing this material also viewed the following: