Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.03775 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.045 g/cc
0.03775 lb/in³
approximation
Struktol STRUKSILON 8027 Silicone Stabilizer for PU-Rigid Foam
STRUKSILON 8027 is a specifically designed silicone stabilizer for appliance application and other applications where good flowability is required, like pipe insulation and hot water boiler producti..
Density 1.045 g/cc
0.03775 lb/in³
ISO 1183
Styrolution Polystyrol 165 H GR 21 PS
Description: Polystyrol 165 H is a high molecular weight, good flowing grade, often blended with high impact extrusion grades.Applications: In blends with high impact Polystyrene or Styrolux; thermo..
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron AP-78 EP ABS Electro Plating Applications
Electroplating & Hot Stamping GradesInformation provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron HI-40 B ABS High Impact Injection Molding
Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron HR-59 ABS Heat Resistant
High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron HR-59(M) ABS Heat Resistant
High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron HR-60 ABS Heat Resistant
High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron IM-14S ABS Very High Rigidity Injection Molding Grade
Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron IM-16M ABS Very High Rigidity Injection Molding Grade
Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron IM-18 ABS Heat Resistant
High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron IM-21 ABS Very High Rigidity Injection Molding Grade
Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron KU-650M ABS Super Heat Resistant
High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron MIF-45 ABS Injection Molding Grade
High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron SE-32M ABS Sheet Extrusion Grade
Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron IM-17A(HF) ABS Injection Molding Grade
Very High Flow, Medium Impact GradeInformation provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron IM-18 ABS Heat Resistant
High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron SE-20P ABS Sheet Extrusion Grade
ABS Pipe GradeInformation provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron TG-3(M) ABS High Impact Injection Molding
Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron IM-29 ABS Injection Molding Grade
High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron SE-22M ABS Sheet Extrusion Grade
Sheet Extrusion grade for profile & DoorsInformation provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron SE-32 ABS Sheet Extrusion Grade
Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron SHF-50+ ABS Injection Molding Grade
High Flow High Gloss, Fancy ApplicationsInformation provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron HI-40 B ABS High Impact Injection Molding
Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron IM-16M ABS Very High Rigidity Injection Molding Grade
Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron SE-22M ABS Sheet Extrusion Grade
Sheet Extrusion grade for profile & DoorsInformation provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron SE-32 ABS Sheet Extrusion Grade
Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron IM-11B ABS Injection Molding Grade
High Impact Strength, Medium Flow, High Fatigue ResistanceInformation provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron SE-45 ABS Sheet Extrusion Grade
Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron IM-17A ABS Injection Molding Grade
Medium Impact, High Gloss, High FlowInformation provided by Bhansali
Density 1.045 g/cc
0.03775 lb/in³
ASTM D-792
Bhansali Engineering Abstron IM-17A(DLW) ABS Injection Molding Grade
Medium Impact, Medium Flow ,White UndertoneInformation provided by Bhansali
Copyright © lookpolymers.com All Rights Reserved