| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.18 g/cc | 0.0426 lb/in³ | ASTM D792 |
| Water Absorption | 1.0 % | 1.0 % | 24 hour immersion; ASTM D570 |
| Linear Mold Shrinkage | 0.0075 cm/cm | 0.0075 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 78 | 78 | ASTM D785 |
| Hardness, Rockwell R | 118 | 118 | ASTM D785 |
| Tensile Strength, Ultimate | 93.1 MPa | 13500 psi | ASTM D638 |
| Elongation at Break | 3.5 % | 3.5 % | ASTM D638 |
| Flexural Strength | 124 MPa | 18000 psi | ASTM D790 |
| Flexural Modulus | 4.10 GPa | 595 ksi | ASTM D790 |
| Compressive Yield Strength | 97.0 MPa | 14100 psi | ASTM D695 |
| Izod Impact, Notched | 1.20 J/cm | 2.25 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 216 °C | 421 °F | ASTM D789 |
| Deflection Temperature at 0.46 MPa (66 psi) | 199 °C | 390 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 188 °C | 370 °F | ASTM D648 |
| Flammability, UL94 | HB | HB |