Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Adell AL-38 Nylon 66, 40% Glass Reinforced; Mineral Filled

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass/Mineral Filled
Manufacturer Adell Plastics, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adell AL-38 Nylon 66, 40% Glass Reinforced; Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ASTM D792
Water Absorption 0.60 %
0.60 %
24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0055 cm/cm
0.0055 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 98
98
ASTM D785
Hardness, Rockwell R 122
122
ASTM D785
Tensile Strength, Ultimate 138 MPa
20000 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Flexural Strength 193 MPa
28000 psi
ASTM D790
Flexural Modulus 7.60 GPa
1100 ksi
ASTM D790
Compressive Yield Strength 255 MPa
37000 psi
ASTM D695
Izod Impact, Notched 0.300 J/cm
0.562 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 263 °C
505 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 249 °C
480 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 246 °C
475 °F
ASTM D648
Flammability, UL94 HB
HB