| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.02 g/cc | 0.0368 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0080 cm/cm | 0.0080 in/in | MD; ASTM D955 |
| Melt Flow | 15 g/10 min | 15 g/10 min | ASTM D1238 |
| Ash | 20 % | 20 % | ASTM D2584 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 45 | 45 | ASTM D785 |
| Tensile Strength at Break | 15.0 MPa | 2180 psi | ASTM D638 |
| Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
| Elongation at Break | 10 % | 10 % | ASTM D638 |
| Elongation at Yield | 3.0 % | 3.0 % | ASTM D638 |
| Tensile Modulus | 1.700 GPa | 246.5 ksi | ASTM D638 |
| Flexural Strength | 22.0 MPa | 3190 psi | ASTM D790 |
| Flexural Modulus | 1.700 GPa | 246.5 ksi | ASTM D790 |
| Izod Impact, Notched | 1.49 J/cm | 2.80 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 103 °C | 217 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 55.0 °C | 131 °F |