Aclo Accutech Polypropylene CP0405UVV Copolymer UV Stabilized

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Aclo Compounders
Trade Name Accutech
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene CP0405UVV Copolymer UV Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Approved to Suzuki PP-S2 Med Grey T01
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Melt Flow 8.0 g/10 min
8.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Elongation at Break 125 %
125 %
ASTM D638
Tensile Modulus 1.500 GPa
217.5 ksi
ASTM D638
Flexural Strength 38.0 MPa
5510 psi
ASTM D790
Flexural Modulus 1.500 GPa
217.5 ksi
ASTM D790
Izod Impact, Notched 1.87 J/cm
3.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 57.8 °C
136 °F
Descriptive Properties Value Comments
Flammability Pass
FMVSS 302
Users viewing this material also viewed the following: