Michelman® Michem® Emulsion 48625M1 Polymer solution

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name Michem® Emulsion
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Emulsion 48625M1 Polymer solution.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Polymer solutionUsage: Michem® Emulsion 48625M1 is a sizing polymer for fiberglass and other fibers serving as reinforcement for various resins.We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint varnishes; floor care; wood finishes; automotive care products; building products; carpets; die lubricants; fruit and vegetable coatings; textiles and urethane foamInformation provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 1.06 - 1.08 g/cc
1.06 - 1.08 g/cc
Volatiles 74 - 76.5 %
74 - 76.5 %
pH 5.0 - 7.0
5.0 - 7.0
Brookfield Viscosity <= 500 cP
<= 500 cP
Spindle # 3, rpm 60
Descriptive Properties Value Comments
Appearance Straw colored liquid
Solids Type BdMA