Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aclo Accutech ABS ABS832G30L Glass Reinforced

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
Manufacturer Aclo Compounders
Trade Name Accutech
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech ABS ABS832G30L Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
MD; ASTM D955
Melt Flow 0.40 g/10 min
0.40 g/10 min
ASTM D1238
Ash 30 %
30 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 103
103
ASTM D785
Tensile Strength at Break 85.98 MPa
12470 psi
ASTM D638
Tensile Strength, Yield 85.98 MPa
12470 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Elongation at Yield 3.0 %
3.0 %
ASTM D638
Tensile Modulus 5.299 GPa
768.6 ksi
ASTM D638
Flexural Strength 134.0 MPa
19430 psi
ASTM D790
Flexural Modulus 8.0986 GPa
1174.6 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 93.9 °C
201 °F
Users viewing this material also viewed the following: