Abatron AboWeld 8708-7 One-Component Structural/Dielectric Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy, Cast, Unreinforced , Epoxy, Thermally Conductive
Manufacturer Abatron
Trade Name AboWeld
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Abatron AboWeld 8708-7 One-Component Structural/Dielectric Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
AboWeld 8708-7 is a highly filled, class H (180°C) structural, heat-conductive adhesive paste for FASTER high-temperature curing. Suggested Uses: Structural bonding; Casting; Potting; Encapsulating; Embedding applications where 2-component systems are not practical; Appliances; Radiators; Electronic components; Medical equipment; Excellent bond to metals, ceramics, glass; Assembly; Patching; Filling; Resurfacing; Insulation.
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0649 lb/in³
Viscosity 1500 cP

@Temperature 100 °C
1500 cP

@Temperature 212 °F
180000 cP

@Temperature 25.0 °C
180000 cP

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D >= 70

@Temperature 120 °C
>= 70

@Temperature 248 °F
90

@Temperature 25.0 °C
90

@Temperature 77.0 °F
Thermal Properties Metric English Comments
CTE, linear 33.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
18.3 µin/in-°F

@Temperature -58.0 - 122 °F
Thermal Conductivity 0.761 W/m-K
5.28 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Dielectric Strength >= 15.7 kV/mm
>= 400 kV/in
Processing Properties Metric English Comments
Cure Time 40.0 min

@Temperature 180 °C
0.667 hour

@Temperature 356 °F
60.0 min

@Temperature 150 °C
1.00 hour

@Temperature 302 °F
180 - 240 min

@Temperature 121 °C
3.00 - 4.00 hour

@Temperature 250 °F
Shelf Life <= 9.00 Month
<= 9.00 Month
Descriptive Properties Value Comments
Color Black
Hardening Time (min) 16
150°C
7
180°C
90
121°C