Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ATI Allvac® Nickelvac® K-500 UNS N05500 Nickel Superalloy

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer ATI Allvac
Trade Name Nickelvac®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® Nickelvac® K-500 UNS N05500 Nickel Superalloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Uses: Pump and drive shafts, impellers, valve components, springs, fasteners, oil well packers, subsurface safety valves.Property values are for samples in the metallurgical condition: 1600°F anneal + water quench + age.Information provided by Allvac, An Allegheny Teledyne Company.
Physical Properties Metric English Comments
Density 8.45 g/cc
0.305 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 27
27
Tensile Strength, Ultimate 1000 MPa
145000 psi
Tensile Strength, Yield 655 MPa

@Strain 0.200 %
95000 psi

@Strain 0.200 %
Elongation at Break 22 %
22 %
Reduction of Area 40 %
40 %
Component Elements Properties Metric English Comments
Aluminum, Al 2.7 %
2.7 %
Carbon, C 0.10 %
0.10 %
Copper, Cu 29 %
29 %
Iron, Fe 1.0 %
1.0 %
Manganese, Mn 0.70 %
0.70 %
Nickel, Ni 66 %
66 %
Silicon, Si 0.25 %
0.25 %
Sulfur, S 0.010 %
0.010 %
Tungsten, W 0.60 %
0.60 %
Users viewing this material also viewed the following: