Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ATI Allegheny Ludlum AL 50™ High Strength Stainless Steel, UNS S20910

Category Metal , Ferrous Metal , Stainless Steel
Manufacturer ATI Allegheny Ludlum
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allegheny Ludlum AL 50™ High Strength Stainless Steel, UNS S20910.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Nitrogen-strengthened austenitic stainless steel for petrochemical, pulp and paper and food processing industries. Available in plate form.Information provided by Allegheny Ludlum
Component Elements Properties Metric English Comments
Chromium, Cr 21 %
21 %
Iron, Fe 63.7 %
63.7 %
as balance
Manganese, Mn 9.0 %
9.0 %
Nickel, Ni 6.0 %
6.0 %
Nitrogen, N 0.30 %
0.30 %
Users viewing this material also viewed the following: