Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Westlake Plastics Absylux® CN-P Acrylonitrile-Butadiene-Styrene (conductive)

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled
Manufacturer Westlake Plastics
Trade Name Absylux®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Absylux® CN-P Acrylonitrile-Butadiene-Styrene (conductive).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Carbon-powder-filled conductive material with high strength and stiffness, and relatively high impact strength. This material is easily machined and fabricated into close tolerance finished parts. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.6 MPa
4000 psi
ASTM D638
Elongation at Break 11 %
11 %
ASTM D638
Flexural Strength 49.6 MPa
7200 psi
ASTM D790
Flexural Modulus 1.93 GPa
280 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Izod Impact, Unnotched 7.21 J/cm
13.5 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 100 - 1.00e+6 ohm-cm
100 - 1.00e+6 ohm-cm
Dry; ASTM D257
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
Dry; ASTM D257
Static Decay <= 0.10 sec
<= 0.10 sec
15% RH; MIL-B-81705-B