3M Dyneon™ TF 9207 PTFE  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ TF 9207 PTFE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Low molecular weight virgin PTFEAgglomerate particlesEasily deagglomeratedInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Bulk Density 0.280 g/cc
0.0101 lb/in³
ASTM D4895
Particle Size 4.0 µm
4.0 µm
average; ISO 13321
120 µm
120 µm
Primary; Dyneon 320
Specific Surface Area 17 m²/g
17 m²/g
BET; DIN 66132
Viscosity 1.00e+6 cP
1.00e+6 cP
Melt
Melt Flow 4.0 g/10 min
4.0 g/10 min