Material Notes:
DescriptionPolypropylene PP 3489-01 is a specially designed homopolymer with excellent stiffness properties. ApplicationTypical applications include high speed extrusion, high speed thin wall injection and fiber applications. PP 3489-01 complies with FDA requirements in 21 CFR 177.1520.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Melt Flow 35 g/10 min
35 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Yield 34.5 MPa
5000 psi
ASTM D638
Elongation at Yield 9.0 %
9.0 %
ASTM D638
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 160 °C
320 °F