Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Advanced Materials PEARLBOND® 500 Linear Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlbond®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials PEARLBOND® 500 Linear Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Pearlbondâ„¢ 500 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a high crystallization rate and a very high thermoplasticity level.Application: Pearlbondâ„¢ 500 can be added to formulations of REACTIVE POLYURETHANE HOT-MELTS (HMPUR), in order to improve the crystallisation speed.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 2781
Viscosity 1.57e+6 cP

@Temperature 130 °C
1.57e+6 cP

@Temperature 266 °F
Melt; ISO 1133
Melt Flow 15 - 30 g/10 min

@Load 2.16 kg,
Temperature 170 °C
15 - 30 g/10 min

@Load 4.76 lb,
Temperature 338 °F
ISO 1133
Thermal Properties Metric English Comments
Melting Point 64.0 - 68.0 °C
147 - 154 °F
MQSA 70 A
Chemical Properties Metric English Comments
Total Base Number <= 3.0
<= 3.0
mg KOH/g; MQSA 47 A
Processing Properties Metric English Comments
Moisture Content <= 0.15 %
<= 0.15 %
MQSA 44
Descriptive Properties Value Comments
Crystallization rate (minutes) 15 - 17
MQSA 12 B
Supply Form Small white pellets
Thermoplasticity Very high
MQSA 68 A