Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Halar® 3404DA Ethylene Chlorotrifluoroethylene Copolymer (ECTFE), Filled

Category Polymer , Thermoplastic , Fluoropolymer , ETFE/ECTFE , ECTFE Fluoropolymer
Manufacturer Solvay Specialty Polymers
Trade Name Halar®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Halar® 3404DA Ethylene Chlorotrifluoroethylene Copolymer (ECTFE), Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Halar® 3404DA is a filled, pearl-white, semicrystalline melt processable fluorinated resin that may be used in full compliance with the federal Food, Drug and Cosmetic Act food additive regulation 21 CFR 177.1380(a)(4). It is designed for electrostatic powder coatings and is particularly recommended for use in protection and anti-corrosion applications where food contact compliance is required.Features: Food Contact Acceptable; Good Chemical Resistance; Good Corrosion Resistance; Good Electrical Properties; Good Surface Finish; Good Thermal Stability; High Hardness; High Purity; Semi CrystallineUses: Coating ApplicationsAdditional Properties: Average Particle Size - Internal Method 28 µmInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
ASTM D1505
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 275 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 527 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 242 °C
468 °F
DSC
Compliance Properties Metric English Comments
FDA Yes
Yes
Descriptive Properties Value Comments
Agency Ratings FDA 21 CFR 177.1380(a)(4)
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color White
Form Powder
Processing Technique Coating