A. Schulman ComAlloy Voloy® 101 Polypropylene, Impact Modified, Flame Retardant, UL

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer A. Schulman ComAlloy
Trade Name Voloy®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF A. Schulman ComAlloy Voloy® 101 Polypropylene, Impact Modified, Flame Retardant, UL.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Ultimate 23.0 MPa
3340 psi
ASTM D638
Elongation at Break 390 %
390 %
ASTM D638
Flexural Strength 33.0 MPa
4790 psi
ASTM D790
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
Izod Impact, Notched 0.750 J/cm
1.41 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
199 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 171 - 195 °C
340 - 383 °F