Material Notes:
Features:easy mold flowexcellent impactgood stiffnessApplications:automotive compoundslawn and garden productsappliancesFormer A-Top Polymers product; part of Amco product line since 2013.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Index of Compound 10 g/10 min

@Temperature 230 °C
10 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.1 MPa
3200 psi
50 mm/min; ASTM D638
Elongation at Yield 6.0 %
6.0 %
50 mm/min; ASTM D638
Flexural Modulus 1.00 GPa
145 ksi
1.3 mm/min, 1% Secant; ASTM D790
Izod Impact, Notched 5.87 J/cm
11.0 ft-lb/in
ASTM D256