| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Middle Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
|
Polymer Resources NY66-G60 Nylon 66, 60% Glass Reinforced
Nylon 66, 60% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test..
|
|||
| Middle Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
|
Polymer Resources NY66-GP1-[color]-H General Purpose Nylon 66, Heat Stabilized
General Purpose Nylon 66, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grad..
|
|||
| Middle Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
|
Polymer Resources NY66-GP1-[color]H Nylon, General Purpose Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Middle Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
|
Polymer Resources NY66-MD1 Nylon 66, 1% MoS2
Nylon 66, 1% Molybdenum Disulfide for Lubrication and WearProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon..
|
|||
| Middle Barrel Temperature | 271 - 310 °C | 520 - 590 °F | |
|
Polymer Resources PPX-G10 Modified-PPO, 10% Glass Reinforced
Modified-Polyphenylene Oxide, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
|
|||
| Middle Barrel Temperature | 271 - 310 °C | 520 - 590 °F | |
|
Polymer Resources PPX-G20 Modified-PPO, 20% Glass Reinforced
Modified-Polyphenylene Oxide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
|
|||
| Middle Barrel Temperature | 271 - 304 °C | 520 - 580 °F | |
|
Polymer Resources PPX-SF2 Modified-PPO, Structural Foam Grade, Flame Retardant
Modified-Polyphenylene Oxide, Structural Foam Grade, Standard FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mec..
|
|||
| Middle Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
|
PTS Tristar® PC-10 10 MFI Extrusion Grade Polycarbonate
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Middle Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
|
Polymer Resources NY66-G55 Nylon 66, 55% Glass Reinforced
Nylon 66, 55% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test..
|
|||
| Middle Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
|
Polymer Resources NY66-IM1 Nylon 66, Medium Impact Modified
Nylon 66, Medium Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are te..
|
|||
| Middle Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
|
Polymer Resources NY66-IM2 Impact Modified Nylon 66
Nylon 66, Superior Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are ..
|
|||
| Middle Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
|
Polymer Resources NY66-MD02-[color]-H Nylon, 2% Molybdenum disulfide for lubrication and wear, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Middle Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
|
Polymer Resources PC-GP3-D-[color]-1 Polycarbonate, General Purpose, High Flow with Mold Release
Polycarbonate, General Purpose, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
|
|||
| Middle Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
|
Polymer Resources PC-UV3-D-[color]-1 Polycarbonate, UV-stabilized, High Flow with Mold Release
Polycarbonate, UV-stabilized, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
|
|||
| Middle Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
|
Samyang Trirex® PC-3025IR 10 MFI Clear Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Middle Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
|
Wellman Wellamid® 220-N Unfilled Nylon 66, Not Lubricated, Nucleated, or Heat Stabilized
Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae..
|
|||
| Middle Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
|
Wellman Wellamid® 22LHI3 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro..
|
|||
| Middle Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
|
Wellman Wellamid® 22LHI4 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro..
|
|||
| Middle Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
|
Wellman Wellamid® GS25-66 22LH-N 25% Glass Sphere Filled Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided..
|
|||
| Middle Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
|
Wellman Wellamid® GS25-66 22L-N, 25% Glass Sphere Filled Nylon 66, Lubricated
Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided..
|
|||
| Middle Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
|
Wellman Wellamid® MRGF25/15 42H-N 25% Mineral/15% Glass Fiber Reinforced Nylon 6, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
|
|||
| Middle Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
|
Wellman Wellamid® MRGF30/10 42H-N 30% Mineral/10% Glass Fiber Reinforced Nylon 6, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
|
|||
| Middle Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
|
Wellman Wellamid® T423-BK10 Mineral Reinforced Nylon 6, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
|
|||
| Middle Barrel Temperature | 271 - 285 °C | 520 - 545 °F | |
|
A. Schulman ComAlloy Lubrilon® 629 Nylon 6/6, Glass Fiber/PTFE Filled, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma..
|
|||
| Middle Barrel Temperature | 271 - 285 °C | 520 - 545 °F | |
|
A. Schulman ComAlloy Voloy® 682 Nylon 6/6, Glass Fiber, Nylon 6/6 Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Middle Barrel Temperature | 271 - 285 °C | 520 - 545 °F | |
|
A. Schulman ComAlloy Voloy® 688 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.45% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod..
|
|||
| Middle Barrel Temperature | 271 - 285 °C | 520 - 545 °F | |
|
A. Schulman ComAlloy Hiloy® 631 Nylon 6/6, Glass Reinforced, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Middle Barrel Temperature | 271 - 285 °C | 520 - 545 °F | |
|
A. Schulman ComAlloy Hiloy® 621 Nylon 6/6, Glass Reinforced
Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Middle Barrel Temperature | 271 - 302 °C | 520 - 575 °F | |
|
Polymer Resources PPX/NY GP2 Modified PPO, Medium Heat PPX/Nylon 6,6 Alloy
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Middle Barrel Temperature | 271 - 310 °C | 520 - 590 °F | |
|
Polymer Resources PPX-GP7 Modified PPO, General Purpose with HDT of 300 F
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||