Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Scotchcal™ 1000-11 Graphic Film

Category Polymer , Film
Manufacturer 3M
Trade Name ScotchCal™
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF 3M Scotchcal™ 1000-11 Graphic Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive adhesive; Confirms a flat surfaces, with and without rivets, moderate compound curves; Permanent filmInformation provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
without adhesive
76.2 - 102 microns
3.00 - 4.00 mil
with adhesive
Mechanical Properties Metric English Comments
Tensile Strength at Break 17.2 MPa
2490 psi
Peel Strength 0.701 kN/m
4.00 pli
Adhesion to ABS
0.701 kN/m
4.00 pli
Adhesion to Acrylic enamel
0.701 kN/m
4.00 pli
Adhesion to Urethane paints
0.877 kN/m
5.00 pli
Adhesion to Chrome
1.40 kN/m
8.00 pli
Adhesion to Aluminum, anodized
Thermal Properties Metric English Comments
Minimum Service Temperature, Air 10.0 °C
50.0 °F
Descriptive Properties Value Comments
Appearance Pearl gray