Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Santoprene® 521-70 Thermoplastic Rubber  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 521-70 Thermoplastic Rubber  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A black thermoplastic elastomer designed for glazing and sealing applications with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be processed using injection molding, extrusion, blow molding or other melt processing techniques.Key Features: Recommended for glazing and sealing applications; Good UV stability; Passes ASTM C 542 Flame Test requirement; Good low temperature flexibilityAdditional processing comments: This thermoplastic rubber is a shear-dependent material that can be processed on conventional thermoplastic equipment for injection molding, extrusion, or blow molding. For extrusion, a general purpose screw with a compression ratio of 2.5 to 3.0 is recommended. Material can be recycled. SANTOPRENE rubber is incompatible with acetal and PVC.Values below are for injection molded plaques, side gated, 82.6 mm x 117.5 mm x 3.0 mm. Tensile properties measured across flow. Data provided by Advanced Elastomer Systems.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
TPE-0105 (ASTM D792)
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
5 Second; TPE-0169 (ASTM D 2240)
Tensile Strength, Ultimate 6.70 MPa
972 psi
TPE-0153 (ASTM D 412)
Elongation at Break 460 %
460 %
TPE-0153 (ASTM D 412)
100% Modulus 0.00380 GPa
0.551 ksi
TPE-0153 (ASTM D 412)
Graves Tear Strength 25.0 kN/m
143 pli
TPE-0056 (ASTM D 624)
Compression Set 37 %

@Temperature 100 °C
37 %

@Temperature 212 °F
168 hrs.; TPE-0016 (ASTM D 412)
Tensile Set 11.5 %
11.5 %
TPE-0053 (ASTM D 412)
Thermal Properties Metric English Comments
Brittleness Temperature <= -57.0 °C
<= -70.6 °F
TPE-0089 (ASTM D 746)
Processing Properties Metric English Comments
Processing Temperature 177 - 232 °C
351 - 450 °F
Drying Temperature 82.0 °C
180 °F
Desiccant drying for 3 hours recommended
Dry Time 3 hour
3 hour