| Category | Ceramic , Oxide , Aluminum Oxide |
| Manufacturer | 3M |
| Trade Name | Nextel™ |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | 3M Nextel™ CF-40 Woven Fabric 550.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 3.03 g/cc | 0.109 lb/in³ | |
| Permeability | 35 | 35 | [ft<sup>3</sup>/min/ft<sup>2</sup>], Air w/o sizing |
| Thickness | 940 microns | 37.0 mil | |
| Fiber Count | 2220 dtex | 2000 denier | 1/2 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 2000 MPa | 290000 psi | filament 25.4mm |
| Tensile Modulus | 193 GPa | 28000 ksi | filament |
| Tear Strength | 45.1 kN/m | 258 pli | Fill, Breaking Strength w/o Sizing |
| 59.8 kN/m | 342 pli | Warp, Breaking Strength w/o Sizing |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 5.30 µm/m-°C @Temperature 100 - 1100 °C |
2.94 µin/in-°F @Temperature 212 - 2010 °F |
|
| Melting Point | 1800 °C | 3270 °F |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.602 | 1.602 |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Al2O3 | 73 % | 73 % | |
| SiO2 | 27 % | 27 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 5.8 @Frequency 9.375e+9 Hz |
5.8 @Frequency 9.375e+9 Hz |