SMAC SMACMOUNT® 2112S 02 Damping Material

Category Other Engineering Material
Manufacturer SMAC
Trade Name SMACMOUNT®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SMAC SMACMOUNT® 2112S 02 Damping Material.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Specifications - Shock & vibration insulation for:Aircraft avionics components & subassembliesMissile electronicsVehicular electronics requiring vibration isolationAdvantages :Bushing style mountCountersunk for lowest installed heightCan be pre-loaded to vary natural frequencyAxial to radial stiffness ratio of approx. 1:1Information provided by SMAC MontBlac Groupe Technologies
Descriptive Properties Value Comments
Load <3.2 kg
1.9 kg
40 Hz, Natural frequency
10 kg
1 mm, Static Deflection
15 kg
2 mm, Static Deflection
3.1 kg
23 Hz, Natural frequency
30 kg
3 mm, Static Deflection
Transmissibility at resonance 0.1
100 Hz
1.1
10.1 Hz
8
20 Hz