3M HQ-115IL Ionic Liquid Precursor

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M HQ-115IL Ionic Liquid Precursor.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Ionic Liquid Precursor HQ-115IL contains the anion bistrifluoromethanesulfonimide (TFSI) which is useful for manufacture of ionic liquids for a variety of applications including polymer antisats, electrolytes and chemical process solvents.Features and Benefits:Hydrophobic: Very low solubility in waterLipophilic: Improved solubility in organic polymersElectrolytic, thermal, UV and hydrolytic stabilityHQ-115IL is an aqueous concentrate for simplified handling and industrial hygiene.HQ-115IL undergoes rapid ion exchange for the manufacture of ionic liquidsInformation provided by 3M
Physical Properties Metric English Comments
Solids Content 78 - 82 %
78 - 82 %
pH 6.0 - 10.5
6.0 - 10.5
Viscosity 16.3 - 16.7 cP
16.3 - 16.7 cP
Thermal Properties Metric English Comments
Boiling Point 139.9 °C

@Pressure 0.101 MPa
283.8 °F

@Pressure 14.7 psi