Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Envision™ 480Cv3 Print Wrap Film

Category Polymer , Film
Manufacturer 3M
Trade Name Envision™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Envision™ 480Cv3 Print Wrap Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High performance, 2-mil white, non-PVC film with a luster finish; Pressure-act adhesive for easy sliding, tacking, snap up and repositioning; non-visible air release channels for fast and easy, bubble-free installations; For inkjet printing with select solvent, eco-solvent, UV and latex inks and for screen priming with select solvent and UV inks. Refer to the Compatible Products and Warranty information sections for the recommended printing platforms; Versatile, ideal for many long-term graphic applications and for short-term wall graphics on smooth or moderately textured surfaces; Flexible, highly conformable over compound curves, corrugations and rivets and requires less heat during application than vinyl films – Stretch graphic construction using selected inks with the 3M™ Envision™ Gloss Wrap Overlaminate 8548G up to 150% ( for example, a 10 inch piece of film can stretch to 15 inches) without primer or relief cuts while maintain lifting resistance; see details and exceptions in Section 9; Removable film, resists tearing in cooler temperature for fast removal; Non-PVC, phthalate-free film; Contains no added chlorine or halogens; Made in part from bio-based materials; Manufactured using 60% less solventInformation provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
without adhesive
76.2 - 102 microns
3.00 - 4.00 mil
with adhesive
Mechanical Properties Metric English Comments
Tensile Strength at Break 37.9 - 44.8 MPa
5500 - 6500 psi
Peel Strength 0.351 - 0.701 kN/m
2.00 - 4.00 pli
Adhesion to ABS
0.351 - 0.701 kN/m
2.00 - 4.00 pli
Adhesion to Acrylic enamel
0.351 - 0.701 kN/m
2.00 - 4.00 pli
Adhesion to Fruehauf pre-painted panels
0.526 - 0.877 kN/m
3.00 - 5.00 pli
Adhesion to Automotive clear coats
0.701 - 1.05 kN/m
4.00 - 6.00 pli
Adhesion to Aluminum, etched
0.877 - 1.23 kN/m
5.00 - 7.00 pli
Adhesion to Aluminum, anodized
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 32.0 °C
89.6 °F
Compound Curves and/or watercraft
38.0 °C
100 °F
Flat without rivets
38.0 °C
100 °F
Curves or corrugations with rivets
38.0 °C
100 °F
Walls
Minimum Service Temperature, Air 4.00 °C
39.2 °F
Flat without rivets
4.00 °C
39.2 °F
Walls
10.0 °C
50.0 °F
Curves or corrugations with rivets
16.0 °C
60.8 °F
Compound Curves and/or watercraft
Copyright © lookpolymers.com All Rights Reserved