3M Controltac™ 8620Cv2 ES Changeable Graphic Film with Comply™ v2 Adhesive

Category Polymer , Film
Manufacturer 3M
Trade Name Controltac™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Controltac™ 8620Cv2 ES Changeable Graphic Film with Comply™ v2 Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
These 2 mil films offer versatility along with sideable, repositionable, pressure activated adhesive. These long term durable and removable films have excellent hiding power and stability, making them perfect for signs and fleet graphics, including surfaces with corrugations and rivets. Use for electrostatic printing. Films 8620C, 8620Cv2 and 8620Cv3 with Comply adhesive have air release channels for fast and easy, bubble-free graphic installations. The air release channels for films with Comply v2 and Comply v3 adhesive are non-visible. The channels in 8620Cv3 also have improved air release.Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
without adhesive
76.2 - 102 microns
3.00 - 4.00 mil
with adhesive
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 17.2 MPa
>= 2490 psi
Peel Strength 0.614 kN/m
3.50 pli
Adhesion to Acrylic enamel
0.701 kN/m
4.00 pli
Adhesion to Fruehauf pre-painted panels
0.736 kN/m
4.20 pli
Adhesion to ABS
0.841 kN/m
4.80 pli
Adhesion to Chrome
0.912 kN/m
5.20 pli
Adhesion to Aluminum, etched
1.38 kN/m
7.90 pli
Adhesion to Aluminum, anodized
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 32.0 °C
89.6 °F
Compound curves
38.0 °C
100 °F
Flat surfaces without rivets
38.0 °C
100 °F
Curved or corrugated surfaces with rivets
Minimum Service Temperature, Air 4.00 °C
39.2 °F
Flat surfaces without rivets
10.0 °C
50.0 °F
Curved or corrugated surfaces with rivets
16.0 °C
60.8 °F
Compound curves