Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Advanced Materials PEARLTHANE® D16N90UV Thermoplastic Polyurethane Elastomer  (discontinued **)

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials PEARLTHANE® D16N90UV Thermoplastic Polyurethane Elastomer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PEARLTHANE® D16N90UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of transparent, colorless pellets, offering adequate hardness, excellent mechanical properties and good hydrolysis and microbial resistance. PEARLTHANE® D16N90UV is designed for extrusion and injection processes.PEARLTHANE® D16N90UV is especially designed for extrusion of tubes and profiles and injection molding of technical parts where excellent mechanical properties at low temperature, hydrolysis and microbe resistance are required.All information provided by Merquinsa
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Melt Flow 10 g/10 min
10 g/10 min
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ASTM D2240
Tensile Strength, Yield 45.0 MPa
6530 psi
ASTM D412
Elongation at Break 450 %
450 %
ASTM D412
100% Modulus 0.00800 GPa
1.16 ksi
ASTM D412
300% Modulus 0.0200 GPa
2.90 ksi
ASTM D412
Tear Strength 130 kN/m
742 pli
ASTM D624 (Die C)
Abrasion 40
40
loss (mm³); DIN 53.516
Thermal Properties Metric English Comments
Melting Point 170 - 180 °C
338 - 356 °F
MQSA 111
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Feed Temperature 195 °C
383 °F
Nozzle Temperature 205 °C
401 °F
Zone 1 210 °C
410 °F
Zone 2 215 - 225 °C
419 - 437 °F
Zone 3 230 - 240 °C
446 - 464 °F
Zone 4 200 - 210 °C
392 - 410 °F
Die Temperature 200 - 210 °C
392 - 410 °F
Mold Temperature 35.0 °C
95.0 °F
Moisture Content <= 0.10 %
<= 0.10 %
MQSA 44
Screw Speed 50 rpm
50 rpm