3M 5690K Silicone Rubber Termination Kits

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF 3M 5690K Silicone Rubber Termination Kits.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ 5630K and 5690K Series Quick Term II Silicone Rubber Termination Kits are one-piece Cold Shrink™ terminations for Tape Shield, Wire Shield and UniShield® power cables. They meet the requirements of IEEE standards 48-1990, for class I terminations. In addition they meet German standard VDE 0278 parts 5 & 100, British standard UNE 21-115-75 and Brazilian standard A-B-N-T-9314. Similar terminations using Quick Term II technology meet French EdF standards HN 33-E-01 and HN 41-E-01. The 3M Quick Term II consists of a high dielectric constant (high-K) stress control tube insulated with a molded silicone skirted insulator. There is a four skirt design rated 15 kV, a six skirt design rated 25/28 kV and eight skirt design rated 34.5 kV. Each insulator design incorporates an extended base feature which when combined with mastic ensures a seal at the cable jacket end where the cable neutral wires are brought out. Quick Term II terminations are provided in an expanded state, mounted on a removable inner supporting plastic core. As supplied in this pre-stretched condition the termination is ready for field installation. During installation the core is unwound, allowing termination to shrink and form a tight seal. Collectively, these termination kits cover cables with primary insulation OD from 0.33” to 1.95” (0.85-49.5 mm) and with cable jacket OD from 0.55”-2.40” (14.0-61.0 mm). These kits can be used to terminate Tape Shield, Wire-Shield and UniShield® power cables from: 8 AWG 5 kV to 1500 kcmil 34.5 kV.Information provided by 3M
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 8.27 MPa
1200 psi
Silicone Rubber Insulator; ASTM D42
9.611 MPa
1394 psi
EPDM Rubber Hi-K Stress Control Tube; ASTM D42
Electrical Properties Metric English Comments
Dielectric Constant 2.7
<br>@Temperature 130 °C
2.7
<br>@Temperature 266 °F
Silicone Rubber Insulator; ASTM D150
3.0
<br>@Temperature 90.0 °C
3.0
<br>@Temperature 194 °F
Silicone Rubber Insulator; ASTM D150
3.4
<br>@Temperature 23.0 °C
3.4
<br>@Temperature 73.4 °F
Silicone Rubber Insulator; ASTM D150
20
<br>@Frequency 100000 Hz
20
<br>@Frequency 100000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
24
<br>@Frequency 10000 Hz
24
<br>@Frequency 10000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
29
<br>@Frequency 1000 Hz
29
<br>@Frequency 1000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
35
<br>@Frequency 150 Hz
35
<br>@Frequency 150 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
24.5
<br>@Frequency 60.0 Hz,<br> Temperature 65.0 °C
24.5
<br>@Frequency 60.0 Hz,<br> Temperature 149 °F
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150
25.2
<br>@Frequency 60.0 Hz,<br> Temperature 90.0 °C
25.2
<br>@Frequency 60.0 Hz,<br> Temperature 194 °F
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150
25.7
<br>@Frequency 60.0 Hz,<br> Temperature 23.0 °C
25.7
<br>@Frequency 60.0 Hz,<br> Temperature 73.4 °F
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150
27.2
<br>@Frequency 60.0 Hz,<br> Temperature 65.0 °C
27.2
<br>@Frequency 60.0 Hz,<br> Temperature 149 °F
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
27.7
<br>@Frequency 60.0 Hz,<br> Temperature 90.0 °C
27.7
<br>@Frequency 60.0 Hz,<br> Temperature 194 °F
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
28.8
<br>@Frequency 60.0 Hz,<br> Temperature 23.0 °C
28.8
<br>@Frequency 60.0 Hz,<br> Temperature 73.4 °F
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
Dielectric Strength 20.0 kV/mm
<br>@Thickness 0.190 mm
507 kV/in
<br>@Thickness 0.00750 in
Silicone Rubber Insulator; ASTM D149
Dissipation Factor 0.12
<br>@Frequency 100000 Hz
0.12
<br>@Frequency 100000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
0.14
<br>@Frequency 10000 Hz
0.14
<br>@Frequency 10000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
0.15
<br>@Frequency 1000 Hz
0.15
<br>@Frequency 1000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
0.16
<br>@Frequency 150 Hz
0.16
<br>@Frequency 150 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
0.093
<br>@Thickness 1650 mm,<br> Frequency 60.0 Hz
0.093
<br>@Thickness 65.0 in,<br> Frequency 60.0 Hz
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150
0.096
<br>@Thickness 584 mm,<br> Frequency 60.0 Hz
0.096
<br>@Thickness 23.0 in,<br> Frequency 60.0 Hz
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150
0.132
<br>@Thickness 2290 mm,<br> Frequency 60.0 Hz
0.132
<br>@Thickness 90.0 in,<br> Frequency 60.0 Hz
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150
0.161
<br>@Thickness 2290 mm,<br> Frequency 60.0 Hz
0.161
<br>@Thickness 90.0 in,<br> Frequency 60.0 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
0.165
<br>@Thickness 1650 mm,<br> Frequency 60.0 Hz
0.165
<br>@Thickness 65.0 in,<br> Frequency 60.0 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
0.166
<br>@Thickness 584 mm,<br> Frequency 60.0 Hz
0.166
<br>@Thickness 23.0 in,<br> Frequency 60.0 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
Track Resistance 3600 sec
3600 sec
3.5 kV; ASTM 2303
36000 sec
36000 sec
2.5 kV; ASTM 2303