| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Track Resistance | 36000 sec | 36000 sec | |
| Glastic 4610-10-E Fiberglass-Reinforced Polyester Standoff Insulator Glastic Standoff Insulators are molded of UL recognized flame resistant fiberglass-reinforced thermoset polyester molding compound. They feature shatter resistance and closer height tolerances than.. |
|||
| Track Resistance | 36000 sec | 36000 sec | |
| Glastic 4640-15 Fiberglass-Reinforced Polyester Standoff Insulator Glastic Standoff Insulators are molded of UL recognized flame resistant fiberglass-reinforced thermoset polyester molding compound. They feature shatter resistance and closer height tolerances than.. |
|||
| Track Resistance | 36000 sec | 36000 sec | 2.5 kV, 10 k Ohms; ASTM 2303-68 |
| 3M 4605 Silicone Rubber Termination Kit 3M™ 4604 and 4605 Quick Term II Silicone Rubber Termination Kits are three-piece Cold Shrink terminations for Tape Shield, Wire Shield, and LC Shield power cables. They meet the requirements of IEE.. |
|||
| Track Resistance | 36000 sec | 36000 sec | 2.5 kV; ASTM 2303 |
| 3M 5360K Silicone Rubber Termination Kits 3M™ 5630K and 5690K Series Quick Term II Silicone Rubber Termination Kits are one-piece Cold Shrink™ terminations for Tape Shield, Wire Shield and UniShield® power cables. They meet the requireme.. |
|||
| Track Resistance | 36000 sec | 36000 sec | 2.5 kV, 10 k Ohms; ASTM 2303-68 |
| 3M 5600 Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink 5600 and 5680 Series QT-II Termination Kits contain one-piece silicone rubber terminations designed for concentric neutral (CN) cable. They meet the requirements of IEEE 48-1990 for.. |
|||
| Track Resistance | 36000 sec | 36000 sec | 2.5 kV; ASTM 2303 |
| 3M 5640 Silicone Rubber Termination Kits 3M™ 5640 and 5650 Series Quick Term II Silicone Rubber Termination Kits are one-piece Cold Shrink™ terminations for Jacketed Concentric Neutral (JCN) power cable. They meet the requirements of IEE.. |
|||
| Track Resistance | 36000 sec | 36000 sec | 2.5 kV; ASTM 2303 |
| 3M 5650 Silicone Rubber Termination Kits 3M™ 5640 and 5650 Series Quick Term II Silicone Rubber Termination Kits are one-piece Cold Shrink™ terminations for Jacketed Concentric Neutral (JCN) power cable. They meet the requirements of IEE.. |
|||
| Track Resistance | 36000 sec | 36000 sec | 2.5 kV, 10 k Ohms; ASTM 2303-68 |
| 3M 5680 Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink 5600 and 5680 Series QT-II Termination Kits contain one-piece silicone rubber terminations designed for concentric neutral (CN) cable. They meet the requirements of IEEE 48-1990 for.. |
|||
| Track Resistance | 36000 sec | 36000 sec | 2.5 kV; ASTM 2303 |
| 3M 5690K Silicone Rubber Termination Kits 3M™ 5630K and 5690K Series Quick Term II Silicone Rubber Termination Kits are one-piece Cold Shrink™ terminations for Tape Shield, Wire Shield and UniShield® power cables. They meet the requireme.. |
|||
| Track Resistance | 36000 sec | 36000 sec | 2.5 kV, 10 k Ohms; ASTM 2303-68 |
| 3M 4604 Silicone Rubber Termination Kit 3M™ 4604 and 4605 Quick Term II Silicone Rubber Termination Kits are three-piece Cold Shrink terminations for Tape Shield, Wire Shield, and LC Shield power cables. They meet the requirements of IEE.. |
|||