3M 4317 Foam Tape

Category Polymer , Tape
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 4317 Foam Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulation. Vinyl foam tapes feature a closed cell design to provide durability, flexibility, weather resistance, and a seal against dust, light, and moisture. Urethane foam tapes have an open cell and include models with excellent cushioning characteristics and high absorbency to trap moisture, dust, and contaminants.Information provided by 3M
Physical Properties Metric English Comments
Density 0.0320 g/cc
0.00116 lb/in³
ASTM D3574
Thickness 9530 microns
375 mil
Mechanical Properties Metric English Comments
Tensile Strength at Break 0.170 MPa
24.7 psi
ASTM D3574
Compressive Strength 0.00207 MPa
0.300 psi
ASTM D3574
Compression Set 5.0 %
5.0 %
ASTM D3574
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 66.0 °C
151 °F
Minimum Service Temperature, Air -29.0 °C
-20.2 °F
Descriptive Properties Value Comments
Adhesive Type Acrylic
Appearance Charcoal Gray