3M 33801 Premium Performance Aluminum Foil Tape

Category Metal , Nonferrous Metal , Aluminum Alloy , Polymer , Tape
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 33801 Premium Performance Aluminum Foil Tape.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High temperature acrylic adhesive of 425°F. UL 723 ClassifiedInformation provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Backing; ASTM D3652
102 microns
4.00 mil
Total; ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 34.3 MPa
4970 psi
ASTM D3759
Peel Strength 0.438 kN/m
2.50 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 218 °C
424 °F
Minimum Service Temperature, Air -34.0 °C
-29.2 °F
Descriptive Properties Value Comments
Adhesive Type Acrylic