Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Manufacturer : Shakespeare Company > Category : Thermoplastic Product List

Tips:Up to 100 items are displayed.
PRODUCT NO. Category Trade Name
Shakespeare AquaBattâ„¢ Staple fiber, denier 16 Thermoplastic AquaBatt™
Shakespeare CL-10XT Super Tough Nylon Copolymer Fishing Line, 10 lb Nylon
Shakespeare CL-10XT Super Tough Nylon Copolymer Fishing Line, 12 lb Nylon
Shakespeare CL-10XT Super Tough Nylon Copolymer Fishing Line, 14 lb Nylon
Shakespeare CL-10XT Super Tough Nylon Copolymer Fishing Line, 17 lb Nylon
Shakespeare CL-10XT Super Tough Nylon Copolymer Fishing Line, 20 lb Nylon
Shakespeare CL-10XT Super Tough Nylon Copolymer Fishing Line, 30 lb Nylon
Shakespeare CL-10XT Super Tough Nylon Copolymer Fishing Line, 4 lb Nylon
Shakespeare CL-10XT Super Tough Nylon Copolymer Fishing Line, 6 lb Nylon
Shakespeare CL-10XT Super Tough Nylon Copolymer Fishing Line, 8 lb Nylon
Shakespeare FGN-11 Nylon 6 Monofilament Nylon 6 Fiber
Shakespeare FGN-12 Nylon 66 Monofilament Nylon 66 Fiber
Shakespeare FL-8 Fluorocarbon PVDF Fishing Line, 12 lb Polyvinylidinefluoride (PVDF), Molded/Extruded
Shakespeare FL-8 Fluorocarbon PVDF Fishing Line, 15 lb Polyvinylidinefluoride (PVDF), Molded/Extruded
Shakespeare FL-8 Fluorocarbon PVDF Fishing Line, 17 lb Polyvinylidinefluoride (PVDF), Molded/Extruded
Shakespeare FL-8 Fluorocarbon PVDF Fishing Line, 20 lb Polyvinylidinefluoride (PVDF), Molded/Extruded
Shakespeare FL-8 Fluorocarbon PVDF Fishing Line, 25 lb Polyvinylidinefluoride (PVDF), Molded/Extruded
Shakespeare FL-8 Fluorocarbon PVDF Fishing Line, 30 lb Polyvinylidinefluoride (PVDF), Molded/Extruded
Shakespeare FL-8 Fluorocarbon PVDF Fishing Line, 6 lb Polyvinylidinefluoride (PVDF), Molded/Extruded
Shakespeare FL-8 Fluorocarbon PVDF Fishing Line, 8 lb Polyvinylidinefluoride (PVDF), Molded/Extruded
Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 10 lb Nylon
Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 100 lb Nylon
Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 12 lb Nylon
Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 130 lb Nylon
Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 14 lb Nylon
Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 15 lb Nylon
Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 17 lb Nylon
Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 20 lb Nylon
Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 25 lb Nylon
Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 30 lb Nylon
Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 35 lb Nylon
Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 4 lb Nylon
Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 40 lb Nylon
Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 50 lb Nylon
Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 6 lb Nylon
Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 60 lb Nylon
Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 8 lb Nylon
Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 80 lb Nylon
Shakespeare HPA-14 diameter 0.7 mm PPS Monofilament Polyphenylene Sulfide (PPS), Unreinforced, Extruded
Shakespeare HPA-30 diameter 0.5 mm PPS Monofilament Polyphenylene Sulfide (PPS), Unreinforced, Extruded
Shakespeare HPA-40 diameter 0.5 mm PPS Monofilament Polyphenylene Sulfide (PPS), Unreinforced, Extruded
Shakespeare HPA-500 diameter 0.9 mm PPS Monofilament Polyphenylene Sulfide (PPS), Unreinforced, Extruded
Shakespeare Isocorâ„¢ 637 Nylon 6 Terpolymer Nylon 6, Unreinforced Isocor™
Shakespeare Isocorâ„¢ 651 Nylon 6 Terpolymer Nylon 6, Unreinforced Isocor™
Shakespeare Isocorâ„¢ 653 Nylon 6 Terpolymer Nylon 6, Unreinforced Isocor™
Shakespeare Isocorâ„¢ CF140ZI Nylon 6/66 Nylon 66/6, Unreinforced Isocor™
Shakespeare Isocorâ„¢ CN30XT Nylon 610 Nylon 610 Isocor™
Shakespeare Isocorâ„¢ CU145SI Nylon 6/66 Nylon 66/6, Unreinforced Isocor™
Shakespeare Isocorâ„¢ HG20SC Nylon 612 Nylon 610, Carbon Fiber Filled Isocor™
Shakespeare Isocorâ„¢ HG26SI medium viscosity PA-612 Nylon 610, Carbon Fiber Filled Isocor™
Shakespeare Isocorâ„¢ HW115SI Nylon 610 Nylon 610 Isocor™
Shakespeare Isocorâ„¢ HZ73SI high viscosity PA-6 Nylon 6, Unreinforced Isocor™
Shakespeare Isocorâ„¢ SC45BT Nylon 610 Nylon 610 Isocor™
Shakespeare Isocorâ„¢ SVP4007 Nylon 6 Nylon 6, Unreinforced Isocor™
Shakespeare Isocorâ„¢ SVP4011 high viscosity PA-6/69 Nylon 6/69 Isocor™
Shakespeare Isocorâ„¢ SVP6100 Nylon 610 Nylon 610 Isocor™
Shakespeare Isocorâ„¢ SVP6104 low viscosity PA-610 Nylon 610 Isocor™
Shakespeare Isocorâ„¢ SVP6105 medium viscosity PA-610 Nylon 610 Isocor™
Shakespeare Isocorâ„¢ TT25TI Nylon 6 Terpolymer Nylon 6, Unreinforced Isocor™
Shakespeare Isocorâ„¢ TT52SI Nylon 6 Terpolymer Nylon 6, Unreinforced Isocor™
Shakespeare Isocorâ„¢ TT65SI Nylon 6 Terpolymer Nylon 6, Unreinforced Isocor™
Shakespeare ISOray Fluoropolymer UV resistant sewing thread, diameter 0.006" Polyvinylidinefluoride (PVDF), Molded/Extruded ISOray
Shakespeare ISOray Fluoropolymer UV resistant sewing thread, diameter 0.008" Polyvinylidinefluoride (PVDF), Molded/Extruded ISOray
Shakespeare ISOray Fluoropolymer UV resistant sewing thread, diameter 0.010" Polyvinylidinefluoride (PVDF), Molded/Extruded ISOray
Shakespeare ISOray Fluoropolymer UV resistant sewing thread, diameter 0.012" Polyvinylidinefluoride (PVDF), Molded/Extruded ISOray
Shakespeare LMX-3 Easy Casting Nylon Copolymer Fishing Line, 10 lb Nylon
Shakespeare LMX-3 Easy Casting Nylon Copolymer Fishing Line, 12 lb Nylon
Shakespeare LMX-3 Easy Casting Nylon Copolymer Fishing Line, 14 lb Nylon
Shakespeare LMX-3 Easy Casting Nylon Copolymer Fishing Line, 15 lb Nylon
Shakespeare LMX-3 Easy Casting Nylon Copolymer Fishing Line, 17 lb Nylon
Shakespeare LMX-3 Easy Casting Nylon Copolymer Fishing Line, 20 lb Nylon
Shakespeare LMX-3 Easy Casting Nylon Copolymer Fishing Line, 8 lb Nylon
Shakespeare MX-200 PP Polypropylene Monofilament Polypropylene, Fiber Grade
Shakespeare MX-201 PP Polypropylene Monofilament Polypropylene, Fiber Grade
Shakespeare MX-229 PVDF Monofilament Polyvinylidinefluoride (PVDF), Molded/Extruded
Shakespeare MX-305 HDPE Monofilament HDPE, Fiber Grade
Shakespeare NX-1037 Nylon 6 Monofilament Nylon 6 Fiber
Shakespeare NX-122 diameter 0.2 mm Nylon Monofilament 610 Nylon 610
Shakespeare NX-152 diameter 0.5 mm Nylon 66 Monofilament Nylon 66 Fiber
Shakespeare NX-201 diameter 0.4 mm Nylon Monofilament 610 Nylon 610
Shakespeare NX-203 diameter 0.2 mm Nylon 6 Monofilament Nylon 6 Fiber
Shakespeare NX-806 Saltwater Nylon Copolymer Fishing Line, 10 lb Nylon
Shakespeare NX-806 Saltwater Nylon Copolymer Fishing Line, 12 lb Nylon
Shakespeare NX-806 Saltwater Nylon Copolymer Fishing Line, 130 lb Nylon
Shakespeare NX-806 Saltwater Nylon Copolymer Fishing Line, 14 lb Nylon
Shakespeare NX-806 Saltwater Nylon Copolymer Fishing Line, 25 lb Nylon
Shakespeare NX-806 Saltwater Nylon Copolymer Fishing Line, 30 lb Nylon
Shakespeare NX-806 Saltwater Nylon Copolymer Fishing Line, 50 lb Nylon
Shakespeare NX-806 Saltwater Nylon Copolymer Fishing Line, 6 lb Nylon
Shakespeare NX-806 Saltwater Nylon Copolymer Fishing Line, 60 lb Nylon
Shakespeare NX-806 Saltwater Nylon Copolymer Fishing Line, 8 lb Nylon
Shakespeare NX-806 Saltwater Nylon Copolymer Fishing Line, 80 lb Nylon
Shakespeare NX-811 Economy Nylon Copolymer Fishing Line, 10 lb Nylon
Shakespeare NX-811 Economy Nylon Copolymer Fishing Line, 12 lb Nylon
Shakespeare NX-811 Economy Nylon Copolymer Fishing Line, 14 lb Nylon
Shakespeare NX-811 Economy Nylon Copolymer Fishing Line, 17 lb Nylon
Shakespeare NX-811 Economy Nylon Copolymer Fishing Line, 20 lb Nylon
Shakespeare NX-811 Economy Nylon Copolymer Fishing Line, 25 lb Nylon
Shakespeare NX-811 Economy Nylon Copolymer Fishing Line, 30 lb Nylon
Shakespeare NX-811 Economy Nylon Copolymer Fishing Line, 4 lb Nylon