Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 10 lb

Category Polymer , Thermoplastic , Nylon
Manufacturer Shakespeare Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 10 lb.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Excellent castability and strength. Economic.Information provided by Shakespeare Company.
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 713.6 MPa
>= 103500 psi
11.7 lb. Minimum Tensile Load 0.012 in. Diameter
Elongation at Break 25 - 35 %
25 - 35 %
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved