Polymer Resources, LTD
Polymer Resources, LTD > ABS Polymer
Manufacturer :
Polymer Resources, LTD
>
Category :
ABS Polymer
Product List
Tips:
Up to 100 items are displayed.
PRODUCT NO.
Category
Trade Name
Polymer Resources ABS-FR Flame Retardant ABS
Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
Polymer Resources ABS-FR-[color]-UV Flame Retardant ABS, UV-stabilized
Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
Polymer Resources ABS-FR1 ABS, Flame Retardant
Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
Polymer Resources ABS-G10 ABS, 10% Glass Reinforced
Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled
Polymer Resources ABS-G30 ABS, 30% Glass Reinforced
Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
Polymer Resources ABS-G5 ABS, 5% Glass Reinforced
Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled
Polymer Resources ABS-G5-[color]-3 ABS, 5% Glass Reinforced, UV-stabilized
Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled
Polymer Resources ABS-GP1 General Purpose ABS
Acrylonitrile Butadiene Styrene (ABS), Molded
Polymer Resources ABS-GP1-[color]-3 ABS, General Purpose, UV-stabilized
Acrylonitrile Butadiene Styrene (ABS), Molded
Polymer Resources ABS-GP1-[color]-EP General Purpose ABS, Electroplating Grade
Acrylonitrile Butadiene Styrene (ABS), Plating Grade
Polymer Resources ABS-GP1-[color]-UV General Purpose ABS, UV-stabilized
Acrylonitrile Butadiene Styrene (ABS), Molded
Polymer Resources ABS-GP-IM General Purpose ABS, Impact Modified
Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Polymer Resources PC/ABS-FR1 Flame Retardant PC/ABS Alloy
Polycarbonate/ABS Alloy, Unreinforced
Polymer Resources PC/ABS-FR1-[color]-WR Flame Retardant PC/ABS Alloy, Wear Resistant
Polycarbonate/ABS Alloy, Unreinforced
Polymer Resources PC/ABS-FR2 Flame Retardant PC/ABS Alloy, High Flow
Polycarbonate/ABS Alloy, Unreinforced
Polymer Resources PC/ABS-FRG5 Flame Retardant PC/ABS Alloy, 5% Glass Reinforced
Polycarbonate/ABS Alloy, Unreinforced
Polymer Resources PC/ABS-G10 General Purpose PC/ABS Alloy, 10% Glass Filled
Polycarbonate/ABS Alloy, Glass Fiber Filled
Polymer Resources PC/ABS-G20 General Purpose PC/ABS Alloy, 20% Glass Filled
Polycarbonate/ABS Alloy, Glass Fiber Filled
Polymer Resources PC/ABS-GP1-[color]-UV General Purpose PC/ABS Alloy, UV-stabilized
Polycarbonate/ABS Alloy, Unreinforced
Polymer Resources PC/ABS-GP2 General Purpose PC/ABS Alloy, High Flow
Polycarbonate/ABS Alloy, Unreinforced
Polymer Resources ABS-G15 ABS, 15% Glass Reinforced
Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
Polymer Resources ABS-G20 ABS, 20% Glass Reinforced
Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
Polymer Resources ABS-G25 ABS, 25% Glass Reinforced
Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
Polymer Resources ABS-GP-HH General Purpose ABS, High Heat
Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
Polymer Resources PC/ABS-FR1-[color]-HH Flame Retardant PC/ABS Alloy, Low Flow
Polycarbonate/ABS Alloy, Unreinforced
Polymer Resources PC/ABS-FR1-[color]-UV Flame Retardant PC/ABS Alloy, UV-stabilized
Polycarbonate/ABS Alloy, Unreinforced
Polymer Resources PC/ABS-G30 General Purpose PC/ABS Alloy, 30% Glass Filled
Polycarbonate/ABS Alloy, Glass Fiber Filled
Polymer Resources PC/ABS-G40 General Purpose PC/ABS Alloy, 40% Glass Filled
Polycarbonate/ABS Alloy, Glass Fiber Filled
Polymer Resources PC/ABS-GP1 General Purpose PC/ABS Alloy
Polycarbonate/ABS Alloy, Unreinforced
Polymer Resources PC/ABS-GP1-[color]-EP General Purpose PC/ABS Alloy, Electroplating Grade
Polycarbonate/ABS Alloy, Unreinforced
Polymer Resources PC/ABS-GP1-[color]-LG General Purpose PC/ABS Alloy, Low Gloss Grade
Polycarbonate/ABS Alloy, Unreinforced