| Daikin DAI-EL T-530 Thermoplastic Elastomer |
Fluoropolymer |
DAI-EL
|
| Daikin NEOFLON AC-5600 PFA Coating Powder, White |
Polyperfluoroalkoxyethylene, Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON AC-5820 PFA Coating Powder, White |
Polyperfluoroalkoxyethylene, Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON AC-5830 PFA Coating Powder, Gray |
Polyperfluoroalkoxyethylene, Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON AF-0012 PFA Film |
Polyperfluoroalkoxyethylene, Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON AF-0025 PFA Film |
Polyperfluoroalkoxyethylene, Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON AF-0100 PFA Film |
Polyperfluoroalkoxyethylene, Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON AF-0250 PFA Film |
Polyperfluoroalkoxyethylene, Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON AF-1000 PFA Film |
Polyperfluoroalkoxyethylene, Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON AF-1150 PFA Film |
Polyperfluoroalkoxyethylene, Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON AF-1500 PFA Film |
Polyperfluoroalkoxyethylene, Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON AF-2400 PFA Film |
Polyperfluoroalkoxyethylene, Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON AP-201SH PFA Semiconductor Grade |
Polyperfluoroalkoxyethylene, Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON AP-210AS PFA Pellets |
Polyperfluoroalkoxyethylene, Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON AP-211SH PFA Semiconductor Grade |
Polyperfluoroalkoxyethylene, Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON AP-221SH PFA Semiconductor Grade |
Polyperfluoroalkoxyethylene, Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON AP-230ASL PFA Pellets |
Polyperfluoroalkoxyethylene, Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON EA-LR43 ETFE Pellets |
Modified ETFE, Unreinforced |
NEOFLON
|
| Daikin NEOFLON EC-6500 ETFE Coating Powder, White |
Modified ETFE, Unreinforced |
NEOFLON
|
| Daikin NEOFLON EC-6520 ETFE Coating Powder, White |
Modified ETFE, Unreinforced |
NEOFLON
|
| Daikin NEOFLON EP-521 ETFE Pellets |
Modified ETFE, Unreinforced |
NEOFLON
|
| Daikin NEOFLON EP-610 ETFE Pellets |
Modified ETFE, Unreinforced |
NEOFLON
|
| Daikin NEOFLON EP-610AS ETFE Pellets |
Modified ETFE, Unreinforced |
NEOFLON
|
| Daikin NEOFLON EPW-1605GN ETFE Liquid Primer, Green |
ETFE/ECTFE |
NEOFLON
|
| Daikin NEOFLON EPW-1606BL ETFE Liquid Primer, Blue |
ETFE/ECTFE |
NEOFLON
|
| Daikin NEOFLON M-300H PCTFE Granular Molding Powder |
Polychlorotrifluoroethylene (PCTFE); Molded |
NEOFLON
|
| Daikin NEOFLON M-300P PCTFE Pellets |
Polychlorotrifluoroethylene (PCTFE); Molded |
NEOFLON
|
| Daikin NEOFLON M-400H PCTFE Granular Molding Powder |
Polychlorotrifluoroethylene (PCTFE); Molded |
NEOFLON
|
| Daikin NEOFLON NC-1500 FEP Coating Powder, White |
Fluorinated Ethylene Propylene (FEP), Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON NC-1539 FEP Coating Powder, Gray |
Fluorinated Ethylene Propylene (FEP), Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON NC-1810 FEP Coating Powder, White |
Fluorinated Ethylene Propylene (FEP), Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON ND-1 FEP Dispersion, Translucent White |
Fluorinated Ethylene Propylene (FEP), Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON ND-2 FEP Dispersion, Milky White |
Fluorinated Ethylene Propylene (FEP), Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON ND-4 FEP Dispersion, Milky White |
Fluorinated Ethylene Propylene (FEP), Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON ND-4GY FEP Dispersion, Gray |
Fluorinated Ethylene Propylene (FEP), Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON NF-0012 FEP Film |
Fluorinated Ethylene Propylene (FEP), Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON NF-0025 FEP Film |
Fluorinated Ethylene Propylene (FEP), Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON NF-0050 FEP Film |
Fluorinated Ethylene Propylene (FEP), Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON NF-0100 FEP Film |
Fluorinated Ethylene Propylene (FEP), Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON NF-0250 FEP Film |
Fluorinated Ethylene Propylene (FEP), Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON NF-0500 FEP Film |
Fluorinated Ethylene Propylene (FEP), Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON NF-1000 FEP Film |
Fluorinated Ethylene Propylene (FEP), Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON NF-1500 FEP Film |
Fluorinated Ethylene Propylene (FEP), Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON NF-2400 FEP Film |
Fluorinated Ethylene Propylene (FEP), Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON NP-101 FEP Pellets |
Fluorinated Ethylene Propylene (FEP), Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON NP-120 FEP Pellets |
Fluorinated Ethylene Propylene (FEP), Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON NP-130 FEP Pellets |
Fluorinated Ethylene Propylene (FEP), Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON NP-21 FEP Pellets |
Fluorinated Ethylene Propylene (FEP), Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON NP-30 FEP Pellets |
Fluorinated Ethylene Propylene (FEP), Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON NP-40 FEP Pellets |
Fluorinated Ethylene Propylene (FEP), Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON RP-4020 EFEP Pellets |
Modified ETFE, Unreinforced |
NEOFLON
|
| Daikin NEOFLON RP-4040 EFEP Pellets |
Modified ETFE, Unreinforced |
NEOFLON
|
| Daikin NEOFLON RP-5000 EFEP Pellets |
Modified ETFE, Unreinforced |
NEOFLON
|
| Daikin NEOFLON RP-5000AS EFEP Pellets |
Modified ETFE, Unreinforced |
NEOFLON
|
| Daikin POLYFLON D-1E PTFE Dispersion |
PTFE |
POLYFLON
|
| Daikin POLYFLON D-2CE PTFE Dispersion |
PTFE |
POLYFLON
|
| Daikin POLYFLON D-2E PTFE Dispersion |
PTFE |
POLYFLON
|
| Daikin POLYFLON F-104 PTFE Fine Powder |
Polytetrafluoroethylene (PTFE), Molded |
POLYFLON
|
| Daikin POLYFLON F-201 PTFE Fine Powder |
Polytetrafluoroethylene (PTFE), Molded |
POLYFLON
|
| Daikin POLYFLON F-205 PTFE Fine Powder |
Polytetrafluoroethylene (PTFE), Molded |
POLYFLON
|
| Daikin POLYFLON F-302 PTFE Fine Powder |
Polytetrafluoroethylene (PTFE), Molded |
POLYFLON
|
| Daikin POLYFLON FA-500 MPA, White Powder |
Thermoplastic |
POLYFLON
|
| Daikin POLYFLON L-2 PTFE Low Polymer, White Fine Powder |
PTFE |
POLYFLON
|
| Daikin POLYFLON L-5F PTFE Low Polymer, White Fine Powder |
PTFE |
POLYFLON
|
| Daikin POLYFLON LDW-40 PTFE Low Polymer, Milky Liquid |
PTFE |
POLYFLON
|
| Daikin POLYFLON M-111 PTFE Molding Powder, Fine Cut |
Polytetrafluoroethylene (PTFE), Molded |
POLYFLON
|
| Daikin POLYFLON M-112 PTFE Molding Powder, Fine Cut |
Polytetrafluoroethylene (PTFE), Molded |
POLYFLON
|
| Daikin POLYFLON M-12 PTFE Molding Powder, Fine Cut |
Polytetrafluoroethylene (PTFE), Molded |
POLYFLON
|
| Daikin POLYFLON M-139 PTFE Molding Powder, Free Flow |
Polytetrafluoroethylene (PTFE), Molded |
POLYFLON
|
| Daikin POLYFLON M-18 PTFE Molding Powder, Fine Cut |
Polytetrafluoroethylene (PTFE), Molded |
POLYFLON
|
| Daikin POLYFLON M-391 PTFE Molding Powder, Free Flow |
Polytetrafluoroethylene (PTFE), Molded |
POLYFLON
|
| Daikin POLYFLON M-392 PTFE Molding Powder, Free Flow |
Polytetrafluoroethylene (PTFE), Molded |
POLYFLON
|
| Daikin POLYFLON M-393 PTFE Molding Powder, Free Flow |
Polytetrafluoroethylene (PTFE), Molded |
POLYFLON
|
| Daikin POLYFLON MG-1030 PTFE 15% Glass Fiber Filled Molding Powder |
Polytetrafluoroethylene (PTFE), Glass Filled, Molded |
POLYFLON
|
| Daikin POLYFLON MG-1040 PTFE 20% Glass Fiber Filled Molding Powder |
Polytetrafluoroethylene (PTFE), Glass Filled, Molded |
POLYFLON
|
| Daikin POLYFLON MG-1040F PTFE 20% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow |
Polytetrafluoroethylene (PTFE), Glass Filled, Molded |
POLYFLON
|
| Daikin POLYFLON MG-1050F PTFE 25% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow |
Polytetrafluoroethylene (PTFE), Glass Filled, Molded |
POLYFLON
|
| Daikin POLYFLON MG-1241 PTFE 20% Glass Fiber and 5% Graphite Filled Molding Powder |
Polytetrafluoroethylene (PTFE), Glass Filled, Molded |
POLYFLON
|
| Daikin POLYFLON MG-1241F PTFE 20% Glass Fiber and 5% Graphite Filled Molding Powder, High Apparent Density, Free Flow |
Polytetrafluoroethylene (PTFE), Glass Filled, Molded |
POLYFLON
|
| Daikin POLYFLON MG-1431 PTFE 15% Glass Fiber and 5% MoS2 Filled Molding Powder |
Polytetrafluoroethylene (PTFE), Glass Filled, Molded |
POLYFLON
|
| Daikin POLYFLON MG-1431F PTFE 20% Glass Fiber and 5% MoS2 Filled Molding Powder, High Apparent Density, Free Flow |
Polytetrafluoroethylene (PTFE), Glass Filled, Molded |
POLYFLON
|
| Daikin POLYFLON MG-2030 PTFE 15% Graphite Filled Molding Powder |
PTFE |
POLYFLON
|
| Daikin POLYFLON MG-2060 PTFE 30% Graphite Filled Molding Powder |
PTFE |
POLYFLON
|
| Daikin POLYFLON MG-6030 PTFE 15% Carbon Fiber Filled Molding Powder |
PTFE |
POLYFLON
|
| Daikin POLYFLON MG-6030F PTFE 15% Carbon Fiber Filled Molding Powder, High Apparent Density, Free Flow |
PTFE |
POLYFLON
|
| Daikin POLYFLON MG-6050 PTFE 25% Carbon Fiber Filled Molding Powder |
PTFE |
POLYFLON
|
| Daikin POLYFLON PA-10L PTFE Paper |
PTFE |
POLYFLON
|
| Daikin POLYFLON PA-5L PTFE Paper |
PTFE |
POLYFLON
|
| Daikin NEOFLON AC-5539 PFA Coating Powder, Gray |
Polyperfluoroalkoxyethylene, Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON ACX-31 PFA Coating Powder, White |
Polyperfluoroalkoxyethylene, Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON ACX-34 PFA Coating Powder, White |
Polyperfluoroalkoxyethylene, Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON AP-201 PFA Pellets |
Polyperfluoroalkoxyethylene, Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON AP-210 PFA Pellets |
Polyperfluoroalkoxyethylene, Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON AP-230 PFA Pellets |
Polyperfluoroalkoxyethylene, Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON AP-231SH PFA Semiconductor Grade |
Polyperfluoroalkoxyethylene, Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON EC-6820 ETFE Coating Powder, White |
Modified ETFE, Unreinforced |
NEOFLON
|
| Daikin NEOFLON EP-620 ETFE Pellets |
Modified ETFE, Unreinforced |
NEOFLON
|
| Daikin NEOFLON NC-1830 FEP Coating Powder, Gray |
Fluorinated Ethylene Propylene (FEP), Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON NP-20 FEP Pellets |
Fluorinated Ethylene Propylene (FEP), Molded/Extruded |
NEOFLON
|
| Daikin NEOFLON NP-3000 FEP Pellets |
Fluorinated Ethylene Propylene (FEP), Molded/Extruded |
NEOFLON
|