Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Daikin NEOFLON NF-2400 FEP Film

Category Polymer , Film , Thermoplastic , Fluoropolymer , FEP , Fluorinated Ethylene Propylene (FEP), Molded/Extruded
Manufacturer Daikin Industries
Trade Name NEOFLON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Daikin NEOFLON NF-2400 FEP Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
NEOFLON FEP films are a high performance film made from NEOFLON FEP resin and have superior reliability and retention of their properties. NEOFLON FEP is applicable in such diversified fields as electrical, chemical, food, and pharmaceutical industries.Information provided by Daikin Industries.
Physical Properties Metric English Comments
Oxygen Transmission 320 cc-mm/m²-24hr-atm
812 cc-mil/100 in²-24hr-atm
at 25°C
Nitrogen Transmission 104 cc-mm/m²-24hr-atm
263 cc-mil/100 in²-24hr-atm
at 25°C
Thickness 2410 microns
95.0 mil
Mechanical Properties Metric English Comments
Coefficient of Friction 0.040 - 0.060
0.040 - 0.060
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
Oxygen Index >= 95 %
>= 95 %
Optical Properties Metric English Comments
Transmission, Visible 92 - 95 %
92 - 95 %
IR Transmittance 95 - 98 %
95 - 98 %
UV Transmittance 91 - 92 %
91 - 92 %
Electrical Properties Metric English Comments
Dielectric Constant 2.0 - 2.2

@Frequency 1000 Hz
2.0 - 2.2

@Frequency 1000 Hz
ASTM D150
2.0 - 2.2

@Frequency 1e+6 Hz
2.0 - 2.2

@Frequency 1e+6 Hz
ASTM D150
Dissipation Factor 0.00010 - 0.00030
0.00010 - 0.00030
Descriptive Properties Value Comments
Roll Length 15 mm
Roll Weight 100 kg
Roll Width 1250 mm
Users viewing this material also viewed the following: