Material Notes:
A lubricated, 5% glass reinforced acetal offering a balance of rigidity, dimensional stability and tensile strength.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 69.0 MPa
10000 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Yield Strength 93.0 MPa
13500 psi
ASTM D790
Flexural Modulus 3.00 GPa
435 ksi
ASTM D790
Izod Impact, Notched 0.630 J/cm
1.18 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 185 °C
365 °F
ASTM D789
Processing Properties Metric English Comments
Melt Temperature 190 °C
374 °F