Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 4.00e+12 ohm-cm @Temperature 23.0 °C |
4.00e+12 ohm-cm @Temperature 73.4 °F |
IEC 60093 |
DuPont Performance Polymers Hytrel® 4069 TPC-ET
(Unverified Data**) Hytrel® 4069 is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injection.. |
|||
Volume Resistivity | 4.00e+12 ohm-cm | 4.00e+12 ohm-cm | DIN 53482 |
Vyncolit X6952 Novolac Phenolic Glass fiber reinforced phenolic molding compound with superior mechanical properties: very high tensile and flexural strength combined with high elongation at break.USES: Information provided by Vyn.. |
|||
Volume Resistivity | <= 4.00e+12 ohm-cm | <= 4.00e+12 ohm-cm | |
Cytec (Conap) RN-1000 / EA-028 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Volume Resistivity | 4.00e+12 ohm-cm | 4.00e+12 ohm-cm | IEC 60093 |
DuPont Performance Polymers Hytrel® 4069 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Volume Resistivity | >= 4.00e+12 ohm-cm | >= 4.00e+12 ohm-cm | |
Epoxy Technology EPO-TEK® 353ND-T Black High Temperature Thixotropic Epoxy Product Description: EPO-TEK® 353ND-T Black is a two component, high temperature, thixotropic epoxy for fiber optic, PCB and various medical applications. Advantages & Application Notes: This produ.. |
|||
Volume Resistivity | >= 4.00e+12 ohm-cm | >= 4.00e+12 ohm-cm | |
Epoxy Technology EPO-TEK® 353ND-T High Temperature Thixotropic Epoxy Product Description: EPO TEK® 353ND-T is a two component, highly thixotropic epoxy with non-flowing properties and high temperature resistance. Advantages & Application Notes: Suitable for fiber op.. |
|||
Volume Resistivity | >= 4.00e+12 ohm-cm | >= 4.00e+12 ohm-cm | |
Epoxy Technology EPO-TEK® 353ND-T1 High Temperature Thixotropic Epoxy Material Description: A two component, thixotropic and high temperature epoxy designed for fiber optic, electronics and medical applications. It is a more viscous alternative to EPO-TEK® 353ND-T.I.. |
|||
Volume Resistivity | >= 4.00e+12 ohm-cm | >= 4.00e+12 ohm-cm | |
Epoxy Technology EPO-TEK® 353ND-T4 Thixotropic Epoxy Product Description: EPO-TEK® 353ND-T4 is a two component, highly thixotropic epoxy with non-flowing properties and high temperature resistance. This is a higher viscosity version of EPO-TEK® 353.. |
|||
Volume Resistivity | >= 4.00e+12 ohm-cm | >= 4.00e+12 ohm-cm | |
Epoxy Technology EPO-TEK® 353ND-T5 High Temperature Thixotropic Epoxy Product Description: EPO-TEK® 353ND-T5 is an intermediate viscosity version of EPO-TEK® 353ND and EPO-TEK® 353ND-T. It was designed for high temperature applications in fiber optics, electronics .. |
|||
Volume Resistivity | >= 4.00e+12 ohm-cm | >= 4.00e+12 ohm-cm | |
Epoxy Technology EPO-TEK® H54 High Temperature Epoxy Product Description: EPO-TEK® H54 is a two component, high Tg, electrically and thermally insulating epoxy adhesive for general bonding and high temperature packaging in medical, hybrid, and optica.. |
|||
Volume Resistivity | 4.00e+12 ohm-cm | 4.00e+12 ohm-cm | IEC 60093 |
BASF Ultramid® T 4381 LDS 10/25% Glass/Mineral Filled PA6/6T (Dry) Description: Ultramid® T 4381 LDS is a semi-crystalline, partially aromatic high temperature polyamide (PA6/6T) for laser direct structuring (LPKFLDS®). As the material is reinforced with 10% fibe.. |
|||
Volume Resistivity | 4.00e+12 ohm-cm | 4.00e+12 ohm-cm | ASTM D257 |
Toyobo PELPRENE™ P48U Polyester TPE, Weather-resistant Features: Polyester TPE, Weather-resistantInformation provided by Toyobo. |