Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI)
(Unverified Data**) Torlon 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon PAI has the hi.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1200-15 Polycarbonate Resin Description: LUPOY PC 1200-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1201-08 Polycarbonate Resin Description: LUPOY PC 1201-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1301-10 Polycarbonate Resin Description: LUPOY PC 1301-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1302-05 Polycarbonate Resin Description: LUPOY 1302-5 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1302-07 Polycarbonate Resin Description: LUPOY PC 1302-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1201-22 Polycarbonate Resin Description: LUPOY PC 1201-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1300-03 Polycarbonate Resin Description: LUPOY PC 1300-03 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1302-10 Polycarbonate Resin Description: LUPOY PC 1302-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1302HP-10 Polycarbonate Resin Description: LUPOY PC 1302HP-10 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1302HP-22 Polycarbonate Resin Description: LUPOY PC 1302HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1303AH-15 Polycarbonate Resin Description: LUPOY PC 1303AH-15 Tint Polycarbonate Resin is designed for injection molding of auto-headlamps. It exhibits an excellent physical property balance of heat resistance, transparency and .. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 res.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI), 30% Glass Fiber Torlon® 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics s.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Styron CALIBREâ„¢ 200-6 Polycarbonate Resin Overview: CALIBREâ„¢ 200-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Styron CALIBREâ„¢ 201-22 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Styron CALIBREâ„¢ 201-22 Polycarbonate Resin Overview: CALIBREâ„¢ 201-22 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Styron CALIBREâ„¢ 2061-15 Polycarbonate CALIBREâ„¢ 2061-15 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Styron CALIBREâ„¢ 2061-22 Polycarbonate CALIBREâ„¢ 2061-22 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Styron CALIBREâ„¢ 301-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Styron CALIBREâ„¢ 303V-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300V-10 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, optical clarity and meets UL94 V-2 rating. CALIBRE 300V series products are avai.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Styron EMERGEâ„¢ 4310-6 Polycarbonate EMERGEâ„¢ PC 4310-6 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Equ.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Styron CALIBREâ„¢ 2061-6 Polycarbonate CALIBREâ„¢ 2061-6 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and .. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Styron CALIBREâ„¢ 302-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Styron CALIBREâ„¢ 302-6 Polycarbonate Resin Overview: CALIBREâ„¢ 300-6 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, and optical clarity as well as high melt strength for blow molding and sheet appli.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Styron CALIBREâ„¢ 303 EP Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Styron CALIBREâ„¢ 303V-6 Polycarbonate Resin Overview: CALIBREâ„¢ 303V-6 Polycarbonate resins offer exceptional impact resistance and heat distortion resistance, and meets UL94 V-2 rating. CALIBRE 303V-6 contains a mold release agent, a UV .. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Styron CALIBREâ„¢ MEGARAD 2081-HD-15 2 Polycarbonate Resin Overview: CALIBREâ„¢ MEGARAD 2081 HD-15 2 polycarbonate resin provides end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed .. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Styron EMERGEâ„¢ 4330-6 Polycarbonate EMERGEâ„¢ PC 4330-6 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information .. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Torlon® 4203 Polyamide-imide (PAI)
(discontinued **) Torlon 4203 is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin for extrusion. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon P.. |