Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.30e+16 ohm-cm | 1.30e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL WCP761 PPE-TPE Flexible Noryl injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain re.. |
|||
Volume Resistivity | 1.30e+16 ohm-cm | 1.30e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL WCP761 PPE-TPE (Asia Pacific) Flexible Noryl injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain re.. |
|||
Volume Resistivity | 1.30e+16 ohm-cm | 1.30e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Volume Resistivity | 1.30e+16 ohm-cm | 1.30e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Volume Resistivity | 1.30e+16 ohm-cm | 1.30e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFFR-4133 is a 33% glass-reinforced, halogen-free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. Th.. |
|||
Volume Resistivity | 1.30e+16 ohm-cm | 1.30e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Volume Resistivity | 1.30e+16 ohm-cm @Thickness 2.00 mm |
1.30e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT 403 G-M50 Heat Resistant and Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.30e+16 ohm-cm @Thickness 2.00 mm |
1.30e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT 403 M-G30 Heat Resistant and Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.30e+16 ohm-cm @Thickness 2.00 mm |
1.30e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G20 272 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.30e+16 ohm-cm @Thickness 2.00 mm |
1.30e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G25 202 Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.30e+16 ohm-cm @Thickness 2.00 mm |
1.30e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G25 211 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.30e+16 ohm-cm @Thickness 2.00 mm |
1.30e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G30 202 Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.30e+16 ohm-cm @Thickness 2.00 mm |
1.30e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G30 211 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.30e+16 ohm-cm @Thickness 2.00 mm |
1.30e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G30 291 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.30e+16 ohm-cm @Thickness 2.00 mm |
1.30e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-MFC-101G30 FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.30e+16 ohm-cm @Thickness 2.00 mm |
1.30e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT 403 M-G50 Heat Resistant and Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.30e+16 ohm-cm @Thickness 2.00 mm |
1.30e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G20 291 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.30e+16 ohm-cm @Thickness 2.00 mm |
1.30e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G25 272 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.30e+16 ohm-cm @Thickness 2.00 mm |
1.30e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G25 291 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.30e+16 ohm-cm @Thickness 2.00 mm |
1.30e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G25 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.30e+16 ohm-cm @Thickness 2.00 mm |
1.30e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G30 272 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.30e+16 ohm-cm @Thickness 2.00 mm |
1.30e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G30 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.30e+16 ohm-cm | 1.30e+16 ohm-cm | ASTM D257 |
BLUESTAR 201-G25202 PBT, 25% Glass Filled Typical Applications: Energy saving lighting, E/E applicationsInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Volume Resistivity | 1.30e+16 ohm-cm | 1.30e+16 ohm-cm | ASTM D257 |
BLUESTAR 201-G30202 PBT, 30% Glass Filled Typical Applications: Energy saving lighting, E/E applicationsInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Volume Resistivity | 1.30e+16 ohm-cm | 1.30e+16 ohm-cm | ASTM D257 |
BLUESTAR 403G-MG30 PBT, 30% Glass Filled Typical Applications: High GWIT, RTI, E/EInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Volume Resistivity | 1.30e+16 ohm-cm | 1.30e+16 ohm-cm | Specimens conditioned for 96 hours at 95°F (35°C) and 90% RH; ASTM D257 |
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA)
(Unverified Data**) Amodel HFFR-4133 is a 33% glass-reinforced, halogen- free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. This .. |