Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 1.00e+11 ohm-cm | >= 1.00e+11 ohm-cm | |
Radici Radiflam® A RV250FR (dry) Nylon 66-25GF Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | ASTM D257 |
Polymer Resources NY6-GP1-[color]-H General Purpose Nylon 6, Heat Stabilized General Purpose Nylon 6, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Radici Radilon® A USZ200 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Radici Radilon® CST 38FL (cond.) Nylon 6/66 Radilon® CS is a range of polyamide 6/66 copolymers obtained through the polymerization of caprolactam and hexamethylendiamine salt with adipic acid.Information provided by Radici group. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Radici Radilon® S 32HS (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Volume Resistivity | >= 1.00e+11 ohm-cm | >= 1.00e+11 ohm-cm | |
Radici Radilon® S 32HS (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Radici Radilon® S RV150 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Volume Resistivity | 1.00e+11 - 1.00e+12 ohm-cm | 1.00e+11 - 1.00e+12 ohm-cm | IEC 60093 |
Raschig Group MELOPAS® 2010 MF Melamine Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | IEC 60093 |
Hexion Bakelite™ PF 2400 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof, UL Listed
(disc Phenolic molding compound, inorganically/organically filled, average heat resistance, increased dimensional stability, dish washer proof, UL listed molding compound 1.5 mm/V-0 (ALL).Application area.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA11 GB30 HS 30% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformation provided by .. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA11 GL8 HS UV Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Graphite Powder Lubricant and UV StabilizerFeatures: Heat Stabilized. Good UV Resistance and LubricatedAppearance: Natural ColorIn.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | IEC 60093 |
Solvay TECHNYL® A 218W V30 Black FA PA66, 30% glass fiber, Conditioned Description: Polyamide 66, reinforced with 30% of glass fiber, for injection molding, heat stabilized, with improved hydrolysis resistance.Available in: EuropeProduct Applications: TECHNYL A 218W V3.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Cotronics Resbond™ 919 High Temperature Ceramic Adhesive, High Resistance |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | conditioned; IEC 60093 |
EMS-Grivory Grivory® EBGM-30 HX PA666-GF30 Product description: Grilon EBGM-30 HX is a specially heat stabilized PA66+PA6 injection molding grade with 30% glass fibers. Grilon EBGM-30 HX has the following important properties: High heat resi.. |
|||
Volume Resistivity | 1.00e+11 - 3.16e+11 ohm-cm | 1.00e+11 - 3.16e+11 ohm-cm | IS 3396-1979 |
Amity Thermosets ATI 172 Phenolic Molding Organic and inorganic Filler, Injection Molded Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackVery soft flow .. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | ASTM D257 |
3M Scotch-Weld™ DP125 Gray Epoxy Adhesive Scotch-Weld epoxy adhesive DP125 Gray is a filled, pigmented version of the Scotch-Weld epoxy adhesive DP125 Translucent and has similar performance and flexibility properties.Information provided b.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Atom Adhesives AA-BOND F131 Epoxy Adhesive AA-BOND F131 is two parts fiber-optic adhesive used for terminating ALL types of fiber-optic connectors as well as LED displays, lenses and other optical components. AA-BOND F131 produces a typical .. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | Conditioned; CEI 60093 |
Addiplast Addinyl C2 M20 V10 Nylon 66/6, Glass/Mineral Filled Mixed products with improved stiffness and good dimensional stability, low warpage.Information provided by Addiplast. |
|||
Volume Resistivity | >= 1.00e+11 ohm-cm | >= 1.00e+11 ohm-cm | |
Radici Radiflam® S RV250FR (dry) Nylon 6 Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro.. |
|||
Volume Resistivity | >= 1.00e+11 ohm-cm | >= 1.00e+11 ohm-cm | |
Radici Radilon® A ESL128 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Volume Resistivity | >= 1.00e+11 ohm-cm | >= 1.00e+11 ohm-cm | |
Radici Radilon® A HSK (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Volume Resistivity | >= 1.00e+11 ohm-cm | >= 1.00e+11 ohm-cm | |
Radici Radilon® A RV300 990 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Radici Radilon® A RV300R (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Volume Resistivity | >= 1.00e+11 ohm-cm | >= 1.00e+11 ohm-cm | |
Radici Radilon® A RV350 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Radici Radilon® S ESL128 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | Conditioned; IEC 60093 |
Solvay Technyl® A 402 H1 Nylon 66 Unreinforced, very high viscosity, heat stabilized, for extrusion and injection molding. TECHNYL® A 402 H1 offers three main advantages: high impact resistance at low humidity levels, good rigidit.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | conditioned; IEC 60093 |
EMS-Grivory Grivory® TS FR PA666 FR Information provided by EMS Grivory |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Radici Radiflam® A RV300AE (cond.) Nylon 66-30GF PA66 flame retardant injection molding grade. 30% Glass fiber reinforced, for items with high stiffness. Natural colorInformation provided by Radici group. |