Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 7.00e+14 ohm-cm | 7.00e+14 ohm-cm | Conditioned; ASTM D257 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better .. |
|||
Volume Resistivity | 7.00e+14 ohm-cm @Temperature 23.0 °C |
7.00e+14 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas.. |
|||
Volume Resistivity | 7.00e+14 ohm-cm | 7.00e+14 ohm-cm | Silicone Rubber; JIS-K-6249/ASTM D257 |
Fujipoly Industries FG-S Connector Fujipoly FG-S connectors have anisotropic conduction properties. The fine metal wires are embedded in a vertical orientation within the silicone rubber width of 0.40mm. Low resistance and high curre.. |
|||
Volume Resistivity | 7.00e+14 ohm-cm | 7.00e+14 ohm-cm | Silicone Rubber; JIS-K-6249/ASTM D257 |
Fujipoly Industries FG-S Fine Connector Fujipoly FG-S connectors have anisotropic conduction properties. The fine metal wires are embedded in a vertical orientation within the silicone rubber width of 0.40mm. Low resistance and high curre.. |
|||
Volume Resistivity | 7.00e+14 ohm-cm | 7.00e+14 ohm-cm | IEC 60093 |
Lanxess Durethan® BKV 35 HTS 901510 Nylon 6, 35% Glass Fiber PA 6, injection molding grade, 35% glass fibers, very good heat-ageing resistance |
|||
Volume Resistivity | 7.00e+14 ohm-cm | 7.00e+14 ohm-cm | IEC 60093 |
Lanxess Durethan® BKV 50 H2.0 EF 900116 Nylon 6, 50% Glass Fiber PA 6, injection molding grade, 50% glass fibers, good heat-ageing resistance, low viscosity (easy flow)Application Examples: mirror baseplates |
|||
Volume Resistivity | 7.00e+14 ohm-cm | 7.00e+14 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |
|||
Volume Resistivity | 7.00e+14 ohm-cm | 7.00e+14 ohm-cm | dry; IEC 60093 |
DSM Novamid® 1015G35 NAT PA6-GF35 35% Glass Reinforced, Injection Molding |
|||
Volume Resistivity | 7.00e+14 ohm-cm | 7.00e+14 ohm-cm | dry; IEC 60093 |
DSM Novamid® 1015GH35 BK37 PA6-GF35 35% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Volume Resistivity | 7.00e+14 ohm-cm | 7.00e+14 ohm-cm | ASTM D1458 |
3M Scotch® 70 HDT Self-Fusing Silicone Rubber Electrical Tape with Tapered Edge Scotch® Silicone Rubber Electrical Tape 70 HDT is a high-temperature arc-and track-resistant tape composed of self-fusing, inorganic silicone rubber and easy-tear and easy-strip liner. The 70 HDT p.. |
|||
Volume Resistivity | 7.00e+14 ohm-cm | 7.00e+14 ohm-cm | Cured property; ASTM D257 |
Aptek DAT-A-THERM 1000 Electrically insulating urethane film DAT-A-THERM 1000 is a tough, flexible, void free, electrically insulating urethane film designed to fill air gaps and dissipate heat between devices and substrates. DAT-A-THERM 1000 film is a 100% s.. |