Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 4.80e+15 ohm-cm | 4.80e+15 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Xenoy® 6370 PBT+PC 30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility. |
|||
Volume Resistivity | 4.80e+15 ohm-cm | 4.80e+15 ohm-cm | |
Tra-Con Tra-Cast 3107 Low Shrinkage Epoxy Casting System TRA-CAST 3107 is a versatile epoxy casting system developed for high performance production potting, encapsulating, casting and tooling applications where low shrinkage, easy handling and flowabilit.. |
|||
Volume Resistivity | 4.80e+15 ohm-cm | 4.80e+15 ohm-cm | |
Dow Corning SILASTIC® 9252/150P A&B KIT 35 Durometer, 2-part, 10 to 1 mix, translucent, Fabric Coating grade, Liquid Silicone RubberInformation provided by Dow Corning |
|||
Volume Resistivity | 4.80e+15 ohm-cm | 4.80e+15 ohm-cm | |
Dow Corning SILASTIC® 9252/250P PARTS A&B Information provided by Dow Corning |
|||
Volume Resistivity | 4.80e+15 ohm-cm | 4.80e+15 ohm-cm | |
Dow Corning SILASTIC® 9280/75E KIT PARTS A&B 60 Durometer, 2-part, 1 to 1 mix, translucent, injection moulding grade, Liquid Silicone Rubber.Information provided by Dow Corning |
|||
Volume Resistivity | 4.80e+15 ohm-cm | 4.80e+15 ohm-cm | ASTM D257 |
ExxonMobil LLDPE LL 1004YB Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 1004YB is a C4 Ziegler Natta LLDPE, especially designed for Low Voltage power cable insulation, using the two-step silane cross-linking process. The grade contains a higher l.. |
|||
Volume Resistivity | 4.80e+15 ohm-cm | 4.80e+15 ohm-cm | ASTM D257 |
3M 7997MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |