Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 100 ohm-cm | >= 100 ohm-cm | ASTM D257 |
Polikim EFALON® K-35 PTFE, 35% Carbon Filled K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings... |
|||
Volume Resistivity | 100 ohm-cm | 100 ohm-cm | 2.5 wt% carbon nanotubes in PC; CTM E043 |
Nanocyl PLASTICYL™ PC1501 Polycarbonate with 2 wt% Multi-Wall Carbon Nanotubes PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |
|||
Volume Resistivity | 100 - 10000 ohm-cm | 100 - 10000 ohm-cm | ASTM D257 |
PolyOne Edgetek® AT-15CF/000 BLACK Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Asia Pacific) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Europe-Africa-Middle East) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Volume Resistivity | 100 - 10000 ohm-cm | 100 - 10000 ohm-cm | ASTM D257 |
PolyOne Stat-Tech™ NN-20CF/000 Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Volume Resistivity | <= 100 ohm-cm | <= 100 ohm-cm | ISO D-257 |
Premix Thermoplastics PRE-ELEC® CP 1316
(discontinued **) PRE-ELEC CP 1316 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resis.. |
|||
Volume Resistivity | 100 - 10000 ohm-cm | 100 - 10000 ohm-cm | ASTM D257 |
PolyOne Edgetek® AS-20CF/000 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Volume Resistivity | 100 ohm-cm | 100 ohm-cm | |
LATI Latishield 66-13A G/30 PA66, Steel/Glass Fiber Reinforced EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON EE003XXC PEI LNP STAT-KON* EE003XXC is a compound based on Polyetherimide resin containing 15% Carbon Fiber. Added features of this material include: Clean Compound System, Electrically Conductive. |
|||
Volume Resistivity | 100 - 10000 ohm-cm | 100 - 10000 ohm-cm | ASTM D257 |
Techmer ES HiFill FR® PA6/6 GF33 FR HS L 15% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 15% Filler by WeightAdditive: LubricantFeatures: Flame Retardant and LubricatedAppearance: BlackInformation.. |
|||
Volume Resistivity | 100 ohm-cm - 1e+05 | 100 ohm-cm - 1e+05 | Dry; ASTM D257 |
Westlake Plastics Absylux® CN-F Acrylonitrile-Butadiene-Styrene (conductive) Non-sloughing, carbon-fiber-filled material with high strength and stiffness; easily machined.Information provided by Westlake Plastics. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | Dry; ASTM D257 |
Westlake Plastics Kynar® PVDF CN-F Polyvinylidene Fluoride (conductive) Non-sloughing carbon-fiber-filled material with resistance to most chemicals and solvents mechanically strong and tough, thermally stable to 335F, flame and abrasion resistant, and easily fabricated.. |
|||
Volume Resistivity | <= 100 ohm-cm | <= 100 ohm-cm | IEC 60093 |
Eurotec® Tecolen® CP20 BK EC PPCP, conductive, black Information provided by Eurotec® |