Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polikim EFALON® K-35 PTFE, 35% Carbon Filled

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Carbon Fiber Filled
Manufacturer Polikim Polimer ve Kimya Sanay
Trade Name EFALON®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Polikim EFALON® K-35 PTFE, 35% Carbon Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings.Information provided by Polikim Polimer.
Physical Properties Metric English Comments
Density 2.00 - 2.10 g/cc
0.0723 - 0.0759 lb/in³
ASTM D792
Deformation 0.30 - 1.8 %
<br>@Temperature 23.0 °C,<br> Time 86400 sec,<br> Pressure 13.7 MPa
0.30 - 1.8 %
<br>@Temperature 73.4 °F,<br> Time 24.0 hour,<br> Pressure 1990 psi
permanent; ASTM D621
1.3 - 1.5 %
<br>@Temperature 150 °C,<br> Time 86400 sec,<br> Pressure 0.981 MPa
1.3 - 1.5 %
<br>@Temperature 302 °F,<br> Time 24.0 hour,<br> Pressure 142 psi
total
2.3 - 4.3 %
<br>@Temperature 23.0 °C,<br> Time 86400 sec,<br> Pressure 13.7 MPa
2.3 - 4.3 %
<br>@Temperature 73.4 °F,<br> Time 24.0 hour,<br> Pressure 1990 psi
total; ASTM D621
5.0 - 6.0 %
<br>@Temperature 150 °C,<br> Time 86400 sec,<br> Pressure 4.90 MPa
5.0 - 6.0 %
<br>@Temperature 302 °F,<br> Time 24.0 hour,<br> Pressure 711 psi
total
Mechanical Properties Metric English Comments
Hardness, Shore D 66 - 70
66 - 70
ASTM D2240
Tensile Strength, Ultimate 10.8 - 15.7 MPa
1560 - 2280 psi
ASTM D638
Elongation at Break 55 - 90 %
55 - 90 %
ASTM D638
Compressive Strength 9.32 - 11.8 MPa
1350 - 1710 psi
1% Deformation; ASTM D695
Coefficient of Friction 0.16
0.16
Coefficient of Friction, Static 0.13
0.13
Limiting Pressure Velocity 0.00360 - 0.00376 MPa-m/sec
103 - 107 psi-ft/min
3 m/min
0.00409 - 0.00654 MPa-m/sec
117 - 187 psi-ft/min
30 m/min
0.004905 - 0.008175 MPa-m/sec
140.0 - 233.4 psi-ft/min
300 m/min
Thermal Properties Metric English Comments
CTE, linear 75.0 - 80.0 µm/m-°C
<br>@Temperature 25.0 - 100 °C
41.7 - 44.4 µin/in-°F
<br>@Temperature 77.0 - 212 °F
ASTM D696
90.0 - 110 µm/m-°C
<br>@Temperature 25.0 - 200 °C
50.0 - 61.1 µin/in-°F
<br>@Temperature 77.0 - 392 °F
ASTM D696
120 - 140 µm/m-°C
<br>@Temperature 25.0 - 300 °C
66.7 - 77.8 µin/in-°F
<br>@Temperature 77.0 - 572 °F
ASTM D696
Thermal Conductivity 0.795 - 0.879 W/m-K
5.51 - 6.09 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 270 °C
518 °F
continuous
Minimum Service Temperature, Air -260 °C
-436 °F
Electrical Properties Metric English Comments
Volume Resistivity >= 100 ohm-cm
>= 100 ohm-cm
ASTM D257
Surface Resistance >= 10000 ohm
>= 10000 ohm
50% rel. humidity; ASTM D257
Copyright © lookpolymers.com All Rights Reserved